11 Years Factory wholesale Nickel Alloy Incoloy 800 UNS N08800 to Madras Manufacturers
continue to improve, to ensure product quality in line with market and customer standard requirements. Our company has a quality assurance system have been established for 11 Years Factory wholesale Nickel Alloy Incoloy 800 UNS N08800 to Madras Manufacturers, we are looking forward to even greater cooperation with overseas customers based on mutual benefits. Please feel free to contact us for more detail
HY 800
Material grades and equivalents
Incoloy 800/GB NS111/UNS N08800/SEW VDIUV W.Nr.1.4876 X10NiCrAlTi3220/BS NA15/AFNOR Z8NC32.21
HY 800 Chemical composition:
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Cu |
S |
Al |
Ti |
800 |
Min. |
30 |
19 |
0.15 |
0.15 |
||||||
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
800H |
Min. |
30 |
19 |
0.05 |
0.15 |
0.15 |
|||||
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
800HT |
Min. |
30 |
19 |
0.06 |
0.15 |
0.15 |
|||||
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
AI+Ti: 0.85-1.20 |
HY 800 Physical properties
Density |
8.0 g/cm³ |
Melting point |
1350-1400 °C |
HY 800 Alloy minimum mechanical properties in the room temperature
Alloy |
Tensile strength |
Yield strength |
Elongation |
Rm N/mm² |
R P 0. 2N/mm² |
A 5 % |
|
800 |
500 |
210 |
35 |
800H |
450 |
180 |
35 |
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
http://www.weldingtipsandtricks.com/metals-and-how-to-weld-nickel.html
How to weld nickel alloys like hastelloy, inconel, etc. Nickel alloys have a low thermal conductivity and so limiting heat input and using lower amperage than would be used for stainless is one key to making good nickel alloy welds.
The progress of improved metallic resources is a crucial action at the leading edge of science and know-how. Metals offer unrivalled mixtures of houses and reliability at a cost which is economical. They are adaptable mainly because subtle improvements in their microstructure can cause dramatic variations in their houses. For illustration, it is feasible to purchase business steel with a energy as lower as 50 MPa or as large as 5500 MPa. They can be built with a microstructure which is finer than that of carbon nanotubes. An understanding of the progress of microstructure in metals, rooted in thermodynamics, crystallography and kinetic phenomena is crucial for the resources scientist. The bulk of the 1.4 billion tonnes of metals made annually are the outcome of developments within just the last 10 a long time
http://www.msm.cam.ac.british isles/phase-trans/2002/creep.1.html