13 Years Factory wholesale Nickel Alloy Incoloy 925 UNS N09925 in Lahore
It adheres to the tenet "Honest, industrious, enterprising, innovative" to develop new products constantly. It regards customers, success as its own success. Let us develop prosperous future hand in hand for 13 Years Factory wholesale Nickel Alloy Incoloy 925 UNS N09925 in Lahore, With the aim of "compete with good quality and develop with creativity" and the service principle of "take customers' demand as orientation", we will earnestly provide qualified products and good service for domestic and international customers.
Y925 Material grades and equivalents
HY 925 /UNSN09925
HY 925 Chemical compostion:
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Cu |
S |
Al |
Ti |
P |
Mo |
HY 925 |
Min. |
42 |
19.5 |
bal |
1.5 |
0.15 |
1.9 |
2.5 |
|||||
Max. |
46 |
23.5 |
0.03 |
1 |
0.5 |
3 |
0.03 |
0.50 |
2.4 |
0.03 |
3.5 |
HY 925 Physical properties:
Density |
8.14 g/cm3 |
Melting point |
1343 ℃ |
HY 925 minimum mechanical properties in the roomtemperature
Alloy state |
Tensile strength |
Yield strength RP0.2 N/mm2 |
Elongation A 5 % |
Solution treatment |
650 |
300 |
30 |
HY 925 Characteristic as below :
This is an age-hardenable alloy of nickel-chromium-iron. The additions of titanium and aluminum enable it to be age-hardened while molybdenum and copper contents enhance resistance to corrosive media. Designed primarily for applications in the production of gas.
HY 925 Application field:
It is used in the petroleum industry for applications such as gas well components, valves and tubing, as well as finding use in high-strength piping systems.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Inconel – Nickel Dependent Super Alloy – 600, 625, 718, X-750 Qualities and Programs August 2013 Inconel is a tremendous alloy and mixes effectively with Copper. Inconel arrives in a lot of varieties: Round Bar, Plate, Sheet, Pipe, Tube. Inconel is hard to machine for the reason that it perform hardens, Inconel 625 can be welded a bit.
Qingdao NPA Marketplace Co. Ltd is a foremost manufacturer specialized in centrifugal casting tube and static castings of warmth resistant alloys, which include ethylene cracking furnace tube, reformer furnace tube, CAL(constant annealing traces) &CGL(constant galvanizing traces) furnace roller and radiant tube, glass lehr roller and warmth/have on resistant castings. The annual potential is 9000 tons centrifugal casting tube and 3500 tons static castings (500 tons precision castings).
Internet site: www.npa-china.com