HY 686 Material grades and equivalents
Inconel 686 / UNS N06686 / Werkstoff Nr.2.4606
HY 686 Chemical composition:
Type |
% Main Chemical Composition % |
||||||||||
Mo |
Cr |
Fe |
W |
C |
Si |
Mn |
P |
S |
Ti |
Ni |
|
HY 686 |
15.0~17.0 |
19.0~23.0 |
≤5.0 |
3.0~4.4 |
≤0.01 |
≤0.08 |
≤0.75 |
≤0.04 |
≤0.02 |
0.02-0.25 |
Rest |
HY 686 Physical properties:
Density | Melting range | Hardness |
8.73 | 1338~1380 | HRC36 |
HY 686 Alloy minimum mechanical properties in the room temperature
Condition |
Tensile Strength |
Yield strength |
Elongation |
Rm N/mm² |
R P 0. 2N/mm² |
A 5 % |
|
Solution |
690 |
380 |
45 |
Cold Drawing/Hot Rolled |
1115 |
1020 |
23.1 |
HY 686 Characteristic as below
HY 686 is solid solution strengthening and corrosion resistance nickel based alloy of NI-Cr-Mo, which has good corrosion resistance in severe corrosive environment. They mainly apply to heat exchanger, reaction container and delivery pipe in the area of chemical processing, processing, pollution control, papermaking, industry and garbage treatment etc.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
http://www.GovLiquidation.com – This 69,560 lbs of Inconel 625 scrap steel has been bought. To look at a current checklist of obtainable scrap steel material, pay a visit to http://bit.ly/jL05Ke currently!
This Inconel was in matrix roll kind and free in pans. This good deal of significant temp alloy scrap steel consisted of Carbon: max .10%, Chromium: min 20% max 23%, Iron: max 5%, Silicon: max .fifty%, Manganese: max .fifty%, Sulfur: max .015%, Phosphorus: max .015%, Molybdenum: min 8% max 10%, Titanium: max .forty%, Nickel: Stability.
This material was positioned in Anniston, AL.
To look at a current checklist of obtainable scrap steel material, pay a visit to http://bit.ly/jL05Ke currently!
I am earning my own wedding day band from Inconel X-750 just to be diverse. The material is a agony to do the job with thanks to the superior nickel/chromium articles. The lathe is a LeBlond “dual generate” with an Aloris-copy device article. I built an adapter for the one.25″ boring bar socket to sleeve it down to a 5/8″ side-lock drill shank. I utilised an indicator to sweep the device holder, inserting it instantly on center. The drill is a Seco CrownLoc As well as with .625″ tip, running at around 80sfm, hand feed with plenty of stress, and drenched in reducing oil (not demonstrated in pic). Chips had been astonishingly limited of course, I had to withdrawal the device numerous moments to eliminate chips, due to the fact they weren’t becoming flushed by coolant.