We have a highly efficient team to deal with inquiries from customers. Our goal is "100% customer satisfaction by our product quality, price & our team service" and enjoy a good reputation among clients. With many factories, we can provide a wide range of 25 Years Factory Iron Alloy Precision Alloy 1J79 Alloy4 to Sweden Factory, We welcome new and old customers from all walks of life to contact us for future business relationships and mutual success!
HY J79 Material grades and equivalents
1J79 / AISI/ASTM Alloy4
HY J79 Chemical composition
Grade |
C |
P |
S |
Mn |
Ni |
Si |
Mo |
Cu |
Fe |
||||
≤ |
|||||||||||||
HY J79 |
0.03 |
0.02 |
0.02 |
0.6-1.1 |
78.5-80.5 |
0.3-0.5 |
3.8-4.1 |
≤0.20 |
Rest |
HY J79 Alloy Mechanical properties in the room temperature
Grade |
Shape |
Magnetic properties |
|||
Initial permeabilityμO |
Maximum permeabilityμm |
Hc |
Saturation induction density BS |
||
HY J79 |
Cold rolling strips |
≥31 |
≥250 |
≤1.2 |
0.75 |
Rod wire |
≥25 |
≥3125 |
≤2.4 |
0.75 |
HY J79 Characteristic as below
HY J79 has a high initial permeability, to work in a weak magnetic field of various transformers, transformers, magnetic amplifiers, choke coil core and magnetic shielding.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Discovery and Science Channel’s How It truly is Designed Alloy Wheels episode.
All copyrights go to their respective homeowners.
Provider foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,3rd Industrial District XiTou Village SongGang City Bao’An District ShenZhen Town GuangDong Province China