Reliable quality and good credit standing are our principles, which will help us at a top-ranking position. Adhering to the tenet of "quality first, customer supreme" for 8 Year Exporter Iron alloy Stainless Steel Nitronic 60 Export to Luxembourg, items won certifications with the regional and international primary authorities .For far more detailed information,please contact us!
HY Nitronic 60 Material grades and equivalents
UNS |
AISI/ASTM |
S21800 |
Alloy218 |
HY Nitronic 60 Chemical composition:
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
N |
P |
S |
HY Nitronic 60 |
Min. |
8 |
16 |
59 |
|
7 |
3.5 |
0.08 |
|
|
Max. |
9 |
18 |
66 |
0.1 |
9 |
4.5 |
0.18 |
0.04 |
0.03 |
HY Nitronic 60 Physical properties
Density |
8.0g/cm3 |
Melting point |
1375°C |
HY Nitronic 60 Alloy minimum mechanical properties in the room temperature
Alloy status |
Tensile strength Rm N/mm² |
Yield strength RP0.2 N/mm² |
Elongation A5 % |
Brinell hardness HB |
Solution treatment |
600 |
320 |
35 |
≤100 |
HY Nitronic 60 Characteristic
HY Nitronic 60 Stainless Steel provides a significantly lower cost way to fight galling and wear compared with cobalt-bearing and high nickel alloys. Its uniform corrosion resistance is better than type 304 in most media. In HY Nitronic 60 ,chloride pitting is superior to Type 316.
Yield strength at room temperature is nearly twice that of 304 and 316.
HY Nitronic 60 provides excellent high temperature oxidation resistance and low-temperature impact resistance.
HY Nitronic 60 Application field:
Used extensively in the Power, Chemical, Petrochemical, Food and Oil & Gas industries with an array of uses including expansion joint wear plates, pump wear rings, bushings, process valve stems, seals and logging equipment.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Qingdao NPA Marketplace Co. Ltd is a foremost manufacturer specialized in centrifugal casting tube and static castings of warmth resistant alloys, which include ethylene cracking furnace tube, reformer furnace tube, CAL(constant annealing traces) &CGL(constant galvanizing traces) furnace roller and radiant tube, glass lehr roller and warmth/have on resistant castings. The annual potential is 9000 tons centrifugal casting tube and 3500 tons static castings (500 tons precision castings).
Internet site: www.npa-china.com
Welding Inconel 718