8 Years Manufacturer Iron Alloy Precision Alloy 1J79 Alloy4 Supply to Toronto
Our goal is to provide high quality products at competitive prices, and top-notch service to customers around the world. We are ISO9001, CE, and GS certified and strictly adhere to their quality specifications for 8 Years Manufacturer Iron Alloy Precision Alloy 1J79 Alloy4 Supply to Toronto, welcomes all overseas friends and merchants to establish collaboration with us. We will provide you with honest, high quality and efficient service to meet your requirements.
HY J79 Material grades and equivalents
1J79 / AISI/ASTM Alloy4
HY J79 Chemical composition
Grade |
C |
P |
S |
Mn |
Ni |
Si |
Mo |
Cu |
Fe |
||||
≤ |
|||||||||||||
HY J79 |
0.03 |
0.02 |
0.02 |
0.6-1.1 |
78.5-80.5 |
0.3-0.5 |
3.8-4.1 |
≤0.20 |
Rest |
HY J79 Alloy Mechanical properties in the room temperature
Grade |
Shape |
Magnetic properties |
|||
Initial permeabilityμO |
Maximum permeabilityμm |
Hc |
Saturation induction density BS |
||
HY J79 |
Cold rolling strips |
≥31 |
≥250 |
≤1.2 |
0.75 |
Rod wire |
≥25 |
≥3125 |
≤2.4 |
0.75 |
HY J79 Characteristic as below
HY J79 has a high initial permeability, to work in a weak magnetic field of various transformers, transformers, magnetic amplifiers, choke coil core and magnetic shielding.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
High successful HRSA turbine blade roughing on Starrag LX 051
- Materials technical specs: Nimonic 80A, NiCr20TiAl (2.4952)
- MMR: sixteen.nine cm3/min
Inconel – Nickel Dependent Super Alloy – 600, 625, 718, X-750 Qualities and Programs August 2013 Inconel is a tremendous alloy and mixes effectively with Copper. Inconel arrives in a lot of varieties: Round Bar, Plate, Sheet, Pipe, Tube. Inconel is hard to machine for the reason that it perform hardens, Inconel 625 can be welded a bit.