Cheap PriceList for Iron Alloy Precision Alloy 4J29 F15 Factory for Calcutta
The key to our success is "Good Product Quality, Reasonable Price and Efficient Service" for Cheap PriceList for Iron Alloy Precision Alloy 4J29 F15 Factory for Calcutta, We sincerely welcome all guests to set up business relationships with us on the basis of mutual benefits. Please contact us now. You will get our professional reply within 8 hours.
HY J29 Material grades and equivalents
4J29/AISI/ASTM F15/JIS EMAS-1001/W.Nr 1.3912
HY J29 Chemical composition
Alloy |
% |
Ni |
Cr |
Fe |
Co |
Cu |
C |
Mn |
Si |
P |
S |
Mo |
HY J29 |
Min |
28.5 |
Rest |
16.8 |
||||||||
Max |
29.5 |
0.2 |
17.8 |
0.20 |
0.03 |
0.50 |
0.30 |
0.02 |
0.02 |
0.20 |
HY J29 Alloy Mechanical properties in the room temperature
Grade |
Average linear expansion factor(10-6℃) |
||||||
20℃~100℃ |
20℃~300℃ |
20℃~400℃ |
20℃~450℃ |
20℃~500℃ |
20℃~530℃ |
20℃~600℃ |
|
HY J29 |
- |
- |
4.6~5.2 |
5.1~5.5 |
- |
- |
- |
HY J29 Characteristic as below
HY J29 having similar coefficient of linear expansion with hard glass within a certain temperature range, applied to vacuum industry to match hard glass.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Discovery and Science Channel’s How It truly is Designed Alloy Wheels episode.
All copyrights go to their respective homeowners.
http://www.GovLiquidation.com – This 69,560 lbs of Inconel 625 scrap steel has been bought. To look at a current checklist of obtainable scrap steel material, pay a visit to http://bit.ly/jL05Ke currently!
This Inconel was in matrix roll kind and free in pans. This good deal of significant temp alloy scrap steel consisted of Carbon: max .10%, Chromium: min 20% max 23%, Iron: max 5%, Silicon: max .fifty%, Manganese: max .fifty%, Sulfur: max .015%, Phosphorus: max .015%, Molybdenum: min 8% max 10%, Titanium: max .forty%, Nickel: Stability.
This material was positioned in Anniston, AL.
To look at a current checklist of obtainable scrap steel material, pay a visit to http://bit.ly/jL05Ke currently!