Cheapest Price Cobalt Alloy Refractaloy 26 UNS R30188 Wholesale to Mecca
We insist on offering high quality production with good business concept, honest sales and the best and fast service. it will bring you not only the high quality product and huge profit, but the most significant is to occupy the endless market for Cheapest Price Cobalt Alloy Refractaloy 26 UNS R30188 Wholesale to Mecca, We are sincerely welcome good friends from numerous circles at dwelling and abroad come to cooperate!
HY R26 Material grades and equivalents
R26/GB GH26/UNS Refractaloy-26/SEW VDIUV W. Nr.1.2888
HY R26 Chemical composition
Alloy |
% |
Ni |
Cr |
Fe |
Mo |
Ti |
Co |
R26 |
Min |
Rest |
|||||
Max |
37 |
18 |
3.0 |
2.7 |
20 |
HY R26 Characteristic
HY R26 has excellent resistance to relaxation, anti creep property, permanence property and resistance to stress corrosion resistance.
Physical properties:
Density:9.14 g/cm3
Melting point:1300℃-1330 ℃
Alloy sheet mechanical properties in the room temperature:
Alloy Status | Tensile strength Rm N/mm2 |
Yield strengthRP0.2 N/mm2 | Elongation A5 % |
Solution Treatment | 925 | 610 | 10 |
HY R26 Application field
HY R26 is a material can be applied in turbine engine blade and fastener.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Inconel – Nickel Dependent Super Alloy – 600, 625, 718, X-750 Qualities and Programs August 2013 Inconel is a tremendous alloy and mixes effectively with Copper. Inconel arrives in a lot of varieties: Round Bar, Plate, Sheet, Pipe, Tube. Inconel is hard to machine for the reason that it perform hardens, Inconel 625 can be welded a bit.