China supplier OEM Iron alloy Stainless Steel 17-4PH for Hongkong Manufacturers

\

Short Introduction:


Product Detail

Product Tags

We have a highly efficient team to deal with inquiries from customers. Our goal is "100% customer satisfaction by our product quality, price & our team service" and enjoy a good reputation among clients. With many factories, we can provide a wide range of China supplier OEM Iron alloy Stainless Steel 17-4PH for Hongkong Manufacturers, we are looking forward to even greater cooperation with overseas customers based on mutual benefits. Please feel free to contact us for more detail


HY 17-4PH Material grades and equivalents

UNS

AISI/ASTM

JIS

W.Nr

S17400

630,17-4PH

SUS630

1.4542

HY 17-4PH Chemical composition:

Alloy

%

Ni

Cr

Fe

C

Mn

Si

S

Cu

Nb

P

HY 17-4PH

Min.

3

15.5

 balance

3

0.15

Max.

5

17.5

0.07

1

1

0.03

5

0.45

0.035

HY 17-4PH Physical properties

Density

7.78/cm3

Melting point

1400-1440 °C

HY 17-4PH Minimum mechanical properties in the room temperature

Status

Tensile strength

Yield strength

Elongation

HRC(HBS)

Rm N/mm²

Rp0.2 N/mm²

A5 %

480°C age

≥1310

≥1180

≥10

≥40

550°C Age

≥1060

≥1000

≥12

≥35

580°C age

≥1000

≥865

≥13

≥31

620°C age

≥930

≥325

≥16

≥28

HY 17-4PH Characteristic:

High strength and hardness, good welding performance and corrosion resistance

HY 17-4PH Application range and field:

Used in components with high strength and corroson resistance

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !