With our excellent management, strong technical capability and strict quality control system, we continue to provide our clients with reliable quality, reasonable prices and excellent services. We aim at becoming one of your most reliable partners and earning your satisfaction for Chinese wholesale Nickel Alloy Incoloy 800 UNS N08800 Supply to Tunisia, we are looking forward to even greater cooperation with overseas customers based on mutual benefits. Please feel free to contact us for more detail
HY 800
Material grades and equivalents
Incoloy 800/GB NS111/UNS N08800/SEW VDIUV W.Nr.1.4876 X10NiCrAlTi3220/BS NA15/AFNOR Z8NC32.21
HY 800 Chemical composition:
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Cu |
S |
Al |
Ti |
800 |
Min. |
30 |
19 |
0.15 |
0.15 |
||||||
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
800H |
Min. |
30 |
19 |
0.05 |
0.15 |
0.15 |
|||||
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
800HT |
Min. |
30 |
19 |
0.06 |
0.15 |
0.15 |
|||||
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
AI+Ti: 0.85-1.20 |
HY 800 Physical properties
Density |
8.0 g/cm3 |
Melting point |
1350-1400 °C |
HY 800 Alloy minimum mechanical properties in the room temperature
Alloy |
Tensile strength |
Yield strength |
Elongation |
Rm N/mm2 |
R P 0. 2N/mm2 |
A 5 % |
|
800 |
500 |
210 |
35 |
800H |
450 |
180 |
35 |
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Discovery and Science Channel’s How It truly is Designed Alloy Wheels episode.
All copyrights go to their respective homeowners.
Melting down 1 gram bars of Silver, Copper, Nickel and Brass with hydrogen and oxygen. Brass is previously an alloy of copper and zinc, and did not soften down effortless as a I figured out from my Brass, Guide and Gunpowder video clip. I then blend the a few workable metals Silver, copper and nickel to generate…….Silvcopickel
SUBSCRIBE: http://comprehensive.sc/1bnslc9
Facebook: http://comprehensive.sc/1dT2aaM
RHNB Vs. Watermelon – http://comprehensive.sc/1bns60F
RHNB Vs. Jello – http://comprehensive.s/1bns0WF RHNB Vs. Elmers Glue – http://comprehensive.sc/1dT1TEM
RHNB Entire Playlist – http://comprehensive.sc/1dT1WjP -Want to ship an object / materials / substance to be RHNB’d or HHO’d? Send Here with a comprehensive credit of your donation! PO Box 21 96 Seymour St. Tonawanda NY 14150 Usa