Cobalt alloys HY ST3/Stellite 3/UNS R30001

\
Loading...

Short Introduction:

HY St 3 /Stellite 3/AWS A5.13 RCoCr-C/UNS R30001 is a range of cobaltchromium alloys designed for wear resistance. It is a completely nonmagnetic and corrosionresistant cobalt alloy. There are a number of Stellite alloys, with various compositions optimised for different uses. Some are formulated to maximize combinations of wear resistance, corrosion resistance, or ability to withstand extreme temperatures.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY St 3 Material grades and equivalents: Stellite 3/AWS A5.13 RCoCr-C/UNS R30001

     

    Chemical composition:

    Brand and No

    Carbon

    Manganese

    Silicon

    Chrom

    Nickel

    Moly

    Tung

    Cobalt 

    Iron

    Other

    stellite 3

    2.00-2.70

    1

    1

    29.0-33.0

    3

     

    11.0-14.0

    Bal.

    3

    P.03MAX

    S.03MAX

     Characteristic as below:

    CoCrWalloy is a range of cobaltchromium alloys designed for wear resistance.

    It is a completely nonmagnetic and corrosionresistant cobalt alloy.

    There are a number of Stellite alloys, with various compositions

    optimised for different uses. Some are formulated to maximize combinations of wear resistance, corrosion resistance, or ability to withstand extreme temperatures.

     Processing conditions and application:

    It can use for valve seat, pump parts, pistons, bushings, nozzles etc.

     

    Regular shape for all kinds of alloys

    Form

    Specification

    Supply Form

    Others

    Sheet

    Thickness:0.40-4.75mm,General Width:1000、1219、1500mm

    Whole Coil or piece of it

    Cold Annealed,Surface 2B、2E

    Plate

    Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled)

    Whole Coil or piece of it

    Single hot rolling,Solid solution annealed state,Surface 1D

    Belt

    Thickness:0.10-3.0mm,Width:50-500mm

    Whole Coil or Specified size

    Cold Annealed,Surface 2B、2E

    Bar & Rod

    Rolled barΦ5-45mm,Length≤1500mm

    Polished Bar(circle、Square)

    Solution annealing,descaling

    Forged barΦ26-245mm,Length≤4000mm

    Weld tube

    Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm

    Base on your requirement

    Seamless Tube

    Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm

    Base on your requirement

    Wire

    Outer diameterΦ0.1-13mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Forged piece

    discs,rings,squares,blocks,slabs

    Base on your requirement

    Steel, Alloy

    Flangs

    All kinds of Flangs

    Base on your requirement

    Steel, Alloy

    Welding Material

    Coil wire Φ0.025mm-1.6mm

    Base on your requirement

    Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.

    Straight WireΦ1.6mm-4.0mm

    Welding rodΦ1.2mm-4.0mm

    Tube

    Elbow, three links, four links, different diameter size

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Explosive bonded laminate

    Raw Sheet Thickness≥2mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy