弹性合金/Elastic Alloy | C | S | P | Mn | Si | Ni | Cr | Ti | Al | Co | Mo | W | Fe | 其它元素 Other | |
不大于(MAX) | |||||||||||||||
3J01 | ≤0.05 | 0.02 | 0.02 | ≤1.00 | ≤0.80 | 34.5~36.5 | 11.5~13.0 | 2.7~3.2 | 1.0~1.8 | - | - | - | 余 Bla. | - | |
3J21 | 0.07~1.2 | 0.015 | 0.015 | 1.70~2.30 | 0.6 | 14.0~16.0 | 19.0~21.0 | - | - | 39~41 | 6.5~7.5 | - | 余 Bla. | - | |
3J53 | ≤0.05 | 0.02 | 0.02 | ≤0.8 | ≤0.8 | 41.5~43 | 5.2~5.8 | 2.3~2.7 | 0.5~0.8 | - | - | - | 余 Bla. | - |