factory low price Iron Alloy Precision Alloy 3J53 to Egypt Manufacturers
The company keeps to the operation concept "scientific management, high quality and efficiency primacy, customer supreme for factory low price Iron Alloy Precision Alloy 3J53 to Egypt Manufacturers, We welcome you to inquire us by call or mail and hope to build a successful and cooperative relationship.
HY J53 Material grades and equivalents: 3J53
HY J53 Chemical composition
Grade |
C |
Si |
Mn |
S |
P |
Cr |
Ni |
Mo |
Al |
Ti |
Fe |
≤ |
|||||||||||
HY J53 |
0.05 |
0.8 |
0.8 |
0.02 |
0.02 |
5.2-5.8 |
41.5-43 |
0.7-0.9 |
0.5-0.8 |
2.3-2.7 |
Rest |
HY J53 Alloy Mechanical properties in the room temperature
Grade |
Condition |
Modulus of elasticity |
Tensile strength b |
Hardness |
HY J53 |
Cold work+age |
176400~191100 |
≥1225 |
350~420 |
HY J53 Characteristic as below
HY J53 has a low temperature coefficient of frequency in the range of -40℃~80℃ for mechanical filter orthography, relay reed, of vibration components.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
http://www.weldingtipsandtricks.com/metals-and-how-to-weld-nickel.html
How to weld nickel alloys like hastelloy, inconel, etc. Nickel alloys have a low thermal conductivity and so limiting heat input and using lower amperage than would be used for stainless is one key to making good nickel alloy welds.