HY 800
Material grades and equivalents
Incoloy 800/GB NS111/UNS N08800/SEW VDIUV W.Nr.1.4876 X10NiCrAlTi3220/BS NA15/AFNOR Z8NC32.21
HY 800 Chemical composition:
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Cu |
S |
Al |
Ti |
800 |
Min. |
30 |
19 |
0.15 |
0.15 |
||||||
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
800H |
Min. |
30 |
19 |
0.05 |
0.15 |
0.15 |
|||||
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
800HT |
Min. |
30 |
19 |
0.06 |
0.15 |
0.15 |
|||||
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
AI+Ti: 0.85-1.20 |
HY 800 Physical properties
Density |
8.0 g/cm3 |
Melting point |
1350-1400 °C |
HY 800 Alloy minimum mechanical properties in the room temperature
Alloy |
Tensile strength |
Yield strength |
Elongation |
Rm N/mm2 |
R P 0. 2N/mm2 |
A 5 % |
|
800 |
500 |
210 |
35 |
800H |
450 |
180 |
35 |
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,Third Industrial District XiTou Village SongGang Town Bao’An District ShenZhen Town GuangDong Province China
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.1,Third Industrial District XiTou Village SongGang Town Bao’An District ShenZhen City GuangDong Province China