Factory wholesale price for Iron Alloy Precision Alloy 4J29 F15 in Serbia
Our company puts emphasis on the management, the introduction of talented personnel, and the construction of staff building, trying hard to improve the quality and liability consciousness of staff members. Our company successfully attained IS9001 Certification and European CE Certification of Factory wholesale price for Iron Alloy Precision Alloy 4J29 F15 in Serbia, winning customers' trust is the gold key to our success! If you are interested in our products, please feel free to visit our web site or contact us.
HY J29 Material grades and equivalents
4J29/AISI/ASTM F15/JIS EMAS-1001/W.Nr 1.3912
HY J29 Chemical composition
Alloy |
% |
Ni |
Cr |
Fe |
Co |
Cu |
C |
Mn |
Si |
P |
S |
Mo |
HY J29 |
Min |
28.5 |
Rest |
16.8 |
||||||||
Max |
29.5 |
0.2 |
17.8 |
0.20 |
0.03 |
0.50 |
0.30 |
0.02 |
0.02 |
0.20 |
HY J29 Alloy Mechanical properties in the room temperature
Grade |
Average linear expansion factor(10-6℃) |
||||||
20℃~100℃ |
20℃~300℃ |
20℃~400℃ |
20℃~450℃ |
20℃~500℃ |
20℃~530℃ |
20℃~600℃ |
|
HY J29 |
- |
- |
4.6~5.2 |
5.1~5.5 |
- |
- |
- |
HY J29 Characteristic as below
HY J29 having similar coefficient of linear expansion with hard glass within a certain temperature range, applied to vacuum industry to match hard glass.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
High successful HRSA turbine blade roughing on Starrag LX 051
- Materials technical specs: Nimonic 80A, NiCr20TiAl (2.4952)
- MMR: sixteen.nine cm3/min
http://www.weldingtipsandtricks.com/metals-and-how-to-weld-nickel.html
How to weld nickel alloys like hastelloy, inconel, etc. Nickel alloys have a low thermal conductivity and so limiting heat input and using lower amperage than would be used for stainless is one key to making good nickel alloy welds.