    硬磁,半硬磁/Hard magnetic, semi hard magnetic C S P Mn Si Ni Cr Co V Mo W Ti Fe 其它元素
    不大于(MAX)
    2J04 ≤0.12 0.02 0.025 ≤0.7 ≤0.7 5.3~6.7 - 44.0~46.0 3.5~4.5 - - - 余 Bla. -
    2J07 ≤0.12 0.02 0.025 ≤0.7 ≤0.7 ≤0.7 - 51.0~53.0 6.5~7.5 - - - 余 Bla. -
    2J09 ≤0.12 0.02 0.025 ≤0.7 ≤0.7 ≤0.7 - 51.0~53.0 8.5~9.5 - - - 余 Bla. -
    2J10 ≤0.12 0.02 0.025 ≤0.7 ≤0.7 ≤0.7 - 51.0~53.0 9.5~10.5 - - - 余 Bla. -
    2J31 ≤0.12 0.02 0.025 ≤0.7 ≤0.7 ≤0.7 - 51.0~53.0 10.8~11.7 - - - 余 Bla. -
    2J53 ≤0.08 0.03 0.03 11.5~12.5 ≤0.5 3.0~4.0 - - - 2.5~3.5 - 0.5~0.8 余 Bla. -
    2J84 ≤0.03 0.02 0.02 0.2 - - 25.5~27.0 14.5~16 - 3.0~3.5 - 0.5~0.8 余 Bla. -
    2J85 ≤0.03 0.02 0.02 0.2 0.8~1.1 - 23.5~25.0 11.5~13 - - - - 余 Bla. -