High quality factory Titanium alloy 6Al-2Sn-4Zr-2Mo UNS R54620 Supply to Vietnam
Our products are widely recognized and trusted by users and can meet continuously changing economic and social needs of High quality factory Titanium alloy 6Al-2Sn-4Zr-2Mo UNS R54620 Supply to Vietnam, If you are interested in any of our products or would like to discuss a custom order, please feel free to contact us. We are looking forward to forming successful business relationships with new clients around the world in the near future.
HY Titanium 6-2-4-2 Material grades and equivalents
6Al-2Sn-4Zr-2Mo, 6-2-4-2 Titanium, 6-2-4-2, UNS R54620
Introduction
A near-alpha alloy, primarily used for high strength and toughness, with good creep resistance up to 1000°F. Forging and machining characteristics similar to those of Ti 6Al-4V. Applications include compressor components, hot airframe skin, and engine afterburner structures. The weld ability of Ti 6-2-4-2 is fair, using AMS 4952 weld wire. Several different treatments are available.
Chemistry Composition
|
Al |
Sn |
Zr |
Mo |
C |
N |
H |
O |
Si |
Fe |
Y |
Others, |
Others, |
Ti |
MIN |
5.5 |
1.8 |
3.6 |
1.8 |
- |
- |
- |
- |
0.06 |
- |
- |
- |
- |
- |
MAX |
6.5 |
2.2 |
4.4 |
2.2 |
0.05 |
0.05 |
0.015 |
0.12 |
0.1 |
0.25 |
0.005 |
0.1 |
0.3 |
Balance |
Features
- Machinability similar to austenitic stainless steels
- Easily welded if proper precautions are taken to prevent oxygen, nitrogen and hydrogen contaminations
- Long term stability for temperatures up to 800°F
Applications
- Compressor discs, blades
- Airframe structure, skin
- Engine afterburner components
- Hush kits
Physical Properties
Density: 0.160 lb/in3
Beta Transus: 1825±25°F
Thermal Conductivity: 4.00 Btu • hr/ft2 • hr°F
Coefficient of Thermal Expansion: 32-212°F 4.3 x10-6 in/in°F
Modulus of Elasticity: 16.5×106 psi
Mechanical Properties
Minimum Tensile Properties, AMS 4919, Duplex Annealed
Thickness, in |
0.025 ≤ 0.062 |
> 0.062 ≤ 1.000 |
> 1.000 ≤ 3.000 |
Tensile Strength, ksi |
135,000 |
135,000 |
135,000 |
0.2% offset Yield Strength, ksi |
125,000 |
125,000 |
125,000 |
Elongation, % |
8 |
10 |
10 |
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Melting down 1 gram bars of Silver, Copper, Nickel and Brass with hydrogen and oxygen. Brass is previously an alloy of copper and zinc, and did not soften down effortless as a I figured out from my Brass, Guide and Gunpowder video clip. I then blend the a few workable metals Silver, copper and nickel to generate…….Silvcopickel
SUBSCRIBE: http://comprehensive.sc/1bnslc9
Facebook: http://comprehensive.sc/1dT2aaM
RHNB Vs. Watermelon – http://comprehensive.sc/1bns60F
RHNB Vs. Jello – http://comprehensive.s/1bns0WF RHNB Vs. Elmers Glue – http://comprehensive.sc/1dT1TEM
RHNB Entire Playlist – http://comprehensive.sc/1dT1WjP -Want to ship an object / materials / substance to be RHNB’d or HHO’d? Send Here with a comprehensive credit of your donation! PO Box 21 96 Seymour St. Tonawanda NY 14150 Usa
» Metal Tubes India is a GOVT. OF INDIA Acknowledged STAR EXPORT Dwelling & PED Accredited Maker
» Metal Tubes India is winner of All India Award for export excellence for 6 Consecutive Many years
» Metal Tubes India is an ISO 9001,ISO 14001,OHSAS 18001 Accredited company, our international CRISIL Ranking is SE 2B
» Metal Tubes India is European Force Machines Directive PED-97/23/EC qualified company
Ni 72., Cr fifteen.5, Fe 8. Mn 1. C .fifteen Cu .5 Si .5 S .015
Significant Efficiency Alloys stocks and produces this grade in the adhering to forms: Bar, wire, sheet, plate, coil, fasteners and forgings. Ask for quote on this grade.
Alloy 600 is a nickel-chromium alloy built for use from cryogenic to elevated temperatures in the selection of 2000 deg F(1093 deg C). The superior nickel material of the alloy allows it to retain substantial resistance less than lessening conditions and makes it resistant to corrosion by a range of natural and inorganic compounds. The nickel material gives it exceptional resistance to chloride-ion pressure-corrosion cracking and also offers exceptional resistance to alkaline options.
Inconel 600 Tube
ASME SB-163 ASME SB-516 ASME SB751 AMS 5580
UNS N06600 also offered in numerous forms like cap, elbow, erw pipes, fasteners, fittings, flange, plate, reducer, spherical bar, seamless pipes, sheet, tee and tube at industrial charge.
+ for extra info & specification about Inconel 600 remember to check out
http://www.steeltubesindia.internet/