Hot sale Factory Nickel Alloy Incoloy 925 UNS N09925 to Rome Importers
continue to improve, to ensure product quality in line with market and customer standard requirements. Our company has a quality assurance system have been established for Hot sale Factory Nickel Alloy Incoloy 925 UNS N09925 to Rome Importers, we are seeking for extensive cooperation with honest customers, achieving a new cause of glory with customers and strategic partners.
Y925 Material grades and equivalents
HY 925 /UNSN09925
HY 925 Chemical compostion:
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Cu |
S |
Al |
Ti |
P |
Mo |
HY 925 |
Min. |
42 |
19.5 |
bal |
1.5 |
0.15 |
1.9 |
2.5 |
|||||
Max. |
46 |
23.5 |
0.03 |
1 |
0.5 |
3 |
0.03 |
0.50 |
2.4 |
0.03 |
3.5 |
HY 925 Physical properties:
Density |
8.14 g/cm3 |
Melting point |
1343 ℃ |
HY 925 minimum mechanical properties in the roomtemperature
Alloy state |
Tensile strength |
Yield strength RP0.2 N/mm² |
Elongation A 5 % |
Solution treatment |
650 |
300 |
30 |
HY 925 Characteristic as below :
This is an age-hardenable alloy of nickel-chromium-iron. The additions of titanium and aluminum enable it to be age-hardened while molybdenum and copper contents enhance resistance to corrosive media. Designed primarily for applications in the production of gas.
HY 925 Application field:
It is used in the petroleum industry for applications such as gas well components, valves and tubing, as well as finding use in high-strength piping systems.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Movie da parte di Costanzo Perico