Hot sale good quality Titanium alloy 6Al-2Sn-4Zr-2Mo UNS R54620 Manufacturer in Maldives
abide by the contract", conforms to the market requirement, joins in the market competition by its high quality as well as provides more comprehensive and excellent service for clients to let them become big winner. The pursue of the company, is the clients' satisfaction for Hot sale good quality Titanium alloy 6Al-2Sn-4Zr-2Mo UNS R54620 Manufacturer in Maldives, We welcome new and old customers from all walks of life to contact us for future business relationships and mutual success!
HY Titanium 6-2-4-2 Material grades and equivalents
6Al-2Sn-4Zr-2Mo, 6-2-4-2 Titanium, 6-2-4-2, UNS R54620
Introduction
A near-alpha alloy, primarily used for high strength and toughness, with good creep resistance up to 1000°F. Forging and machining characteristics similar to those of Ti 6Al-4V. Applications include compressor components, hot airframe skin, and engine afterburner structures. The weld ability of Ti 6-2-4-2 is fair, using AMS 4952 weld wire. Several different treatments are available.
Chemistry Composition
Al |
Sn |
Zr |
Mo |
C |
N |
H |
O |
Si |
Fe |
Y |
Others, |
Others, |
Ti |
|
MIN |
5.5 |
1.8 |
3.6 |
1.8 |
- |
- |
- |
- |
0.06 |
- |
- |
- |
- |
- |
MAX |
6.5 |
2.2 |
4.4 |
2.2 |
0.05 |
0.05 |
0.015 |
0.12 |
0.1 |
0.25 |
0.005 |
0.1 |
0.3 |
Balance |
Features
Machinability similar to austenitic stainless steelsEasily welded if proper precautions are taken to prevent oxygen, nitrogen and hydrogen contaminationsLong term stability for temperatures up to 800°F
Applications
Compressor discs, bladesAirframe structure, skinEngine afterburner componentsHush kits
Physical Properties
Density: 0.160 lb/in3
Beta Transus: 1825±25°F
Thermal Conductivity: 4.00 Btu hr/ft2 hr°F
Coefficient of Thermal Expansion: 32-212°F 4.3 x10-6 in/in°F
Modulus of Elasticity: 16.5×106 psi
Mechanical Properties
Minimum Tensile Properties, AMS 4919, Duplex Annealed
Thickness, in |
0.025 ≤ 0.062 |
> 0.062 ≤ 1.000 |
> 1.000 ≤ 3.000 |
Tensile Strength, ksi |
135,000 |
135,000 |
135,000 |
0.2% offset Yield Strength, ksi |
125,000 |
125,000 |
125,000 |
Elongation, % |
8 |
10 |
10 |
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Qingdao NPA Marketplace Co. Ltd is a foremost manufacturer specialized in centrifugal casting tube and static castings of warmth resistant alloys, which include ethylene cracking furnace tube, reformer furnace tube, CAL(constant annealing traces) &CGL(constant galvanizing traces) furnace roller and radiant tube, glass lehr roller and warmth/have on resistant castings. The annual potential is 9000 tons centrifugal casting tube and 3500 tons static castings (500 tons precision castings).
Internet site: www.npa-china.com