Nickel Alloy Incoloy 800HT UNS N08811

\
Loading...

Short Introduction:

HY 800HT/Incoloy 800HT/ UNS N08811/W.Nr.1.4959 X 8 NiCrAlTi 32-21/BS NA 15 (HT) is face-centered cubic lattice structure. very low carbon centent and increased Ti:C rate improve the stability of the structure, anti-allergy , and anti-intergranular corrosion. Low temperature annealing of 950℃ ensure the fine grain structure.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY 800HT

    Material grades and equivalents

    Incoloy 800HT/ UNS N08811/W.Nr.1.4959 X 8 NiCrAlTi 32-21/BS NA 15 (HT)

    Incoloy 800H Chemical composition:

    Alloy

    %

    Ni

    Cr

    Fe

    C

    Mn

    Si

    Cu

    S

    Al

    Ti

    800

    Min.

    30

    19

    0.15

    0.15

    Max.

    35

    23

    balance

    0.1

    1.5

    1

    0.75

    0.015

    0.6

    0.6

    800H

    Min.

    30

    19

    0.05

    0.15

    0.15

    Max.

    35

    23

    balance

    0.1

    1.5

    1

    0.75

    0.015

    0.6

    0.6

    800HT

    Min.

    30

    19

    0.06

    0.15

    0.15

    Max.

    35

    23

    balance

    0.1

    1.5

    1

    0.75

    0.015

    0.6

    0.6

    AI+Ti: 0.85-1.20

    Incoloy 800H Physical properties

    Density

    8.0 g/cm³

    Melting point

    1350-1400 ℃

    Incoloy 800H Alloy minimum mechanical properties in the room temperature

    Alloy

    Tensile strength

    Yield strength

    Elongation

    Rm N/mm²

    R P 0. 2N/mm²

    A 5 %

    800

    500

    210

    35

    800H

    450

    180

    35

    800H Characteristic as below:
    1.Excellent corrosion resistance in the water media of the extremely high temperature of 500℃.
    2.Good stress corrosion resistance
    3.Good machining

    HY 800HTMetallurgical structure:
    800H is face-centered cubic lattice structure. very low carbon centent and increased Ti:C rate
    improve the stability of the structure, anti-allergy , and anti-intergranular corrosion. Low temperature annealing of 950℃ ensure the fine grain structure.

    HY 800HTCorrosion resistance:
    800H can not be corroded in many kinds of media. Its high nickel content made it have good stress corrosion resistance cracking property in the water corrosion condition.High Chromium content made it can better resist pitting and crevice corrosion cracking. This alloy can resist nitric acid and organic acid corrosion, but it is not so fine in the sulfuric acid and hydrochloric acid.
    800H not only good corrosion resistance in both oxidation and non-oxidizing salt, maybe a little pitting in halide, but also very good corrosion resistance property in the mixture of water,smoke, steam,air and carbon dioxide.

    HY 800HTApplication range and field
    1.Nitrate condenser—Corrosion resistance of nitrc acid
    2.Steam heating pipes–Very good mechanical property
    3.Heat up element tube–Very good mechanical property

    For the application of up to 500℃ enviornment, alloy supply state change to annealing.

     

    Specifications:

    Rod, Bar, Wire, Forgings, and Forging Stock

    ASTM B 408 & ASME SB 408;ASTM B 564 & ASME SB 564;ASME Code Case 1325;ASME Code Case 1949;ISO 9723;ISO 9724;ISO 9725;BS 3076NA15;BS 3075NA15;SEW 470;VdTÜV 412 & 434;DIN 17460;EN 10095

    Plate, Sheet, and Strip

    ASTM A 240/A 480;ASME SA 240/SA 480;ASTM B 409/B 906;ASME SB 409/SB 906;ASME Code Case 1325;ASME Code Case 2339;BS 3072NA15;BS 3073NA15;SEW 470;VdTÜV 412 & 434;DIN 17460;EN 10028-7 & EN 10095     

    Pipe & Tube

    ASTM B 163;ASME SB 163;ASTM B 407/B 829;ASME SB 407/SB 829;ASTM B 514/B 775;ASME SB 514/SB 775;ASTM B 515/B 751;ASME SB 515/SB 751;ASME Code Case 1325 and 1983;BS 3074NA15;SEW 470;VdTÜV 412 & 434;ISO 6207;DIN 17459

    Fittings

    ASTM B 366/ASME SB 366

     

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy



  • Previous:
  • Next:

  • Write your message here and send it to us

    RELATED PRODUCTS

    WhatsApp Online Chat !