HY 825/Incoloy 825/GB NS1402/UNS N08825/SEW VDIUV W.Nr.2.4858 NiCr21Mo/BS NA16/AFNOR NC21FeDU is an all-purpose project alloy, have good corrosion resistance of the acid and alkali metal property in both oxidation and reduction environments. High nickel content made it with effective stress corrosion cracking resistance performance. 825 have excellent corrosion resistance in different kinds of media, such as sulfuric acid, phosphoric acid, nitric acid and organic acid, alkali metal such as sodium hydroxide, potassium hydroxide, and hydrochloric acid. A variety of media corrosion of nuclear-burning dissolver show 825 high integrated prpperty, like sulfuric acid, nitric acid and potassium hydroxide are all dealing in a same device. 


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY 825

    Material grades and equivalents

    Incoloy 825/GB NS1402/UNS N08825/SEW VDIUV W.Nr.2.4858 NiCr21Mo/BS NA16/AFNOR NC21FeDU

    HY 825Chemical composition

    Alloy

    %

    Ni

    Cr

    Fe

    C

    Mn

    Si

    Cu

    Mo

    Al

    Ti

    P

    S

    825

    Min.

    38

    19.5

    balance

    1.5

    2.5

    1.0

    0.6

    Max.

    46

    23.5

    balance

    0.05

    1

    0.5

    3

    3.5

    0.2

    1.2

    0.02

    0.03

    HY 825Physical properties

    Density

    8.1 g/cm³

    Melting point

    1370-1400°C

    HY 825Alloy mi nimum mechanical properties in the room temperature

    Alloy state

    Tensile strength
    Rm N/mm²

    Yield strength
    R P0. 2N/mm²

    Elongation
    A 5 %

    Brinell hardness
    HB

    825

    550

    220

    30

    ≤200

     Characteristic as below 

    1. Good stress corrosion cracking resistance performance
    2. Good resistance for pitting and crevice corrosion performance
    3. Good anti-oxidation and non-oxidzing heat acid performance
    4. Good mechanical performance in both room temperature and up to 550°C
    5. Have the pressure vessel authenticate when manufacture temperature up to 450°C

     HY 825Metallurgical structure

    825 is the face-centered cubic lattice structure.

     HY 825Corrosion resistance

    825 is an all-purpose project alloy, have good corrosion resistance of the acid and alkali metal property in both oxidation and reduction environments. High nickel content made it with effective stress corrosion cracking resistance performance. 825 have excellent corrosion resistance in different kinds of media, such as sulfuric acid, phosphoric acid, nitric acid and organic acid, alkali metal such as sodium hydroxide, potassium hydroxide, and hydrochloric acid. A variety of media corrosion of nuclear-burning dissolver show 825 high integrated prpperty, like sulfuric acid, nitric acid and potassium hydroxide are all dealing in a same device.

     HY 825Application field

    825widely use in many kinds of industry field that the working temperature no more than 550°C.

     HY 825Typical application field

    1. Sulfuric acid factory usage for heating pipe, container, basket, chain and so on.
    2. Cooling heat exchanger, marine product pipeline system and gas pipeline of acidic environment.
    3. Heat exchanger, steam machine, washing, impregnation pipe, etc. for phosphoric acid produce
    4. Oil refining in the air heat exchanger
    5. Food project
    6. Chemical process
    7. Application of high pressure oxygen flam-retardant alloy

     

    Specifications:

    Rod, Bar, Wire and Forging Stock

    BS 3076NA16;ASTM B 425;ASTM B 564;ASME SB 425;ASME SB 564;ASME Code Case N-572;DIN 17752;DIN 17753;DIN 17754;VdTÜV 432;ISO 9723;ISO 9724;ISO 9725

    Plate, Sheet and Strip

    BS 3072NA16;BS 3073NA16;ASTM B 424;ASTM B 906;ASME SB 424;ASME SB 906;DIN 17750;VdTÜV 432;ISO 6208

    Pipe & Tube

    BS 3074NA16;ASTM B 163;ASTM B 423;ASTM B 704;ASTM B 705;ASTM B 751;ASTM B 775;ASTM B 829;ASME SB 163;ASME SB 423;ASME SB 704;ASME SB 705;ASME SB 751;ASME SB 775;ASME SB 829;ASME Code Case 1936;DIN 17751;VdTÜV 432 ISO 6207 

     

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy



  • Previous:
  • Next:

  • Write your message here and send it to us

    RELATED PRODUCTS

    WhatsApp Online Chat !