Nickel Alloy Inconel 686 UNS N06686

\
Loading...

Short Introduction:

HY 686 / Inconel 686 / UNS N06686 / Werkstoff Nr.2.4606 is solid solution strengthening and corrosion resistance nickel based alloy of NI-Cr-Mo, which has good corrosion resistance in severe corrosive environment. They mainly apply to heat exchanger, reaction container and delivery pipe in the area of chemical processing, processing, pollution control, papermaking, industry and garbage treatment etc.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY 686 Material grades and equivalents

    Inconel 686 / UNS N06686 / Werkstoff Nr.2.4606

    HY 686 Chemical composition:

    Type

    % Main Chemical Composition %

    Mo

    Cr

    Fe

    W

    C

    Si

    Mn

    P

    S

    Ti

    Ni

    HY 686

    15.0~17.0

    19.0~23.0

    ≤5.0

    3.0~4.4

    ≤0.01

    ≤0.08

    ≤0.75

    ≤0.04

    ≤0.02

    0.02-0.25

    Rest

    HY 686 Physical properties

    Density Melting range Hardness
    8.73 1338~1380 HRC36

    HY 686 Alloy minimum mechanical properties in the room temperature

    Condition

    Tensile Strength

    Yield strength

    Elongation

    Rm N/mm²

    R P 0. 2N/mm²

    A 5 %

    Solution

    690

    380

    45

    Cold Drawing/Hot Rolled

    1115

    1020

    23.1

    HY 686 Characteristic as below

    HY 686 is solid solution strengthening and corrosion resistance nickel based alloy of NI-Cr-Mo, which has good corrosion resistance in severe corrosive environment. They mainly apply to heat exchanger, reaction container and delivery pipe in the area of chemical processing, processing, pollution control, papermaking, industry and garbage treatment etc.

     

    Specifications:

    Rod and Bar

    ASTM B-574;ASME SB-574;VdTÜV 515,12.98;DIN 17752

    Wire

    ASTM B-574;ASME SB-574; DIN 17753

    Plate, Sheet & Strip

    ASTM B-575;ASME SB-575;VdTÜV 515,12.98;DIN 17750

    Forging

    ASTM B-564;ASME SB-564;DIN 17754

    Seamless Tube & Pipe

    ASTM B-622/B 829*;ASME SB-622/SB-829*;VdTÜV 515,1298;DIN 17751

    Welded Tube/pipe

    ASTM B-626/B-751*; ASME SB-626/ SB-751*;ASTM B-619/B-775*; ASME SB-619/SB-775*

     

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy



  • Previous:
  • Next:

  • Write your message here and send it to us

    RELATED PRODUCTS

    WhatsApp Online Chat !