Iron alloy Stainless Steel 17-4PH

\
Loading...

Short Introduction:

HY 17-4PH/S17400/SUS630/1.4542 has high strength and hardness, good welding performance and corrosion resistance.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY 17-4PH Material grades and equivalents

    UNS

    AISI/ASTM

    JIS

    W.Nr

    S17400

    630,17-4PH

    SUS630

    1.4542

    HY 17-4PH Chemical composition:

    Alloy

    %

    Ni

    Cr

    Fe

    C

    Mn

    Si

    S

    Cu

    Nb

    P

    HY 17-4PH

    Min.

    3

    15.5

     balance

    3

    0.15

    Max.

    5

    17.5

    0.07

    1

    1

    0.03

    5

    0.45

    0.035

    HY 17-4PH Physical properties

    Density

    7.78/cm3

    Melting point

    1400-1440 °C

    HY 17-4PH Minimum mechanical properties in the room temperature

    Status

    Tensile strength

    Yield strength

    Elongation

    HRC(HBS)

    Rm N/mm²

    Rp0.2 N/mm²

    A5 %

    480°C age

    ≥1310

    ≥1180

    ≥10

    ≥40

    550°C Age

    ≥1060

    ≥1000

    ≥12

    ≥35

    580°C age

    ≥1000

    ≥865

    ≥13

    ≥31

    620°C age

    ≥930

    ≥325

    ≥16

    ≥28

    HY 17-4PH Characteristic:

    High strength and hardness, good welding performance and corrosion resistance

    HY 17-4PH Application range and field:

    Used in components with high strength and corroson resistance

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy



  • Previous:
  • Next:

  • Write your message here and send it to us

    RELATED PRODUCTS

    WhatsApp Online Chat !