Nickel Alloy Hastelloy C UNS N06003

\

Short Introduction:

HY HC/HastelloyC/GB NS333&NS3303/SEW VDIUV W.Nr.2.4819/BS NA45  is a omnipotent of nickel, chromium and molybdenum mixed alloy, with better corrosion resistance performance than other alloys, for example, Hastelloy C276 alloy, C4 alloy and 625 alloy.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY HC Chemical composition

    Alloy

    %

    Ni

    Cr

    Mo

    Fe

    W

    Co

    C

    Mn

    Si

    V

    P

    S

    C

    Min.

    balance

    14.5

    15

    4

    3

    Max.

    16.5

    17

    7

    4.5

    2.5

    0.08

    1

    1

    0.35

    0.04

    0.03

    C22

    Min.

    balance

    20

    12.5

    2

    2.5

    Max.

    22.5

    14.5

    6

    3.5

    2.5

    0.02

    0.5

    0.08

    0.35

    0.02

    0.02

    HY HC  Physical properties

    Density

    8.9 g/cm³

    Melting point

    1325-1370 °C

    HY HC  Alloy minimum mechanical properties in the room temperature

    Alloy

    Tensile Strength
    Rm N/mm²

    Yield strength
    R P 0. 2N/mm²

        Elongation

    A 5 %

    HY HC

    690

    283

    40

    Characteristic as below  

    HY HC is a omnipotent of nickel, chromium and molybdenum mixed alloy, with better corrosion resistance performance than other alloys, for example, Hastelloy C276 alloy, C4 alloy and 625 alloy. HY HC have a good resistance performance to pitting, crevice corrosion and stress corrosion cracking, have excellent inoxidability water medium performance, including the wet-chlorine, nitric acid or oxidizing acid mixed acid with chloride ion. Meantime, HY HC possesses perfect resistance to reduction and oxidation of processing enviroments, then it can be used in some complicated environment or with many different manufacture target factory depend on the omnipotent performance. HY HC possess prominent resistance performance to different chemical environments, including strong oxidizing matter, such as iron chloride, copper chloride, chlorine, heat pollution liquid(organic and inorganic), formic acid, acetic acid, acetyl oxide, sea water and salting liquid and so on.
    HY HC Metallurgical structure
    HY HC is face-centered cubic lattice structure.
    HY HC Corrosion resistance
    HY HC alloy suit for many kinds of chemical process industry which contain the oxidizing medium and reductant. High molybdenum and chromium content make it can resist the chloride corrosion, and tungsten make this corrosion resistance better. HY HC is one of a few material that can resist the corrosion of moist chlorine, hypochlorite and chlorine dioxide, this alloyhave prominent corrosion resistanceto high concentration chlorate( iron chloride and copper chloride)
    HY HC Application field
    HY HC is widely used in the chemical field and petrifaction field, such as the element of chloride organic and catalyze system. This material especially suit for high temperature environments, impure inorganic acid and organic acid (such as formic acid and acetic acid), sea-water corrosion environments.

    HY HC Other application field
    1. Acetic acid/acetyl oxide
    2.Acid dipping
    3.Cellophane paper manufactures
    4.Chloride system
    5. Complicated mixed acid
    6. Electrogalvanizing groove roller
    7.Expansion bellows
    8.Flue gas washer system
    9.Geothermal well
    10.Fluorine hydride furnace cleaner
    11.Incineration cleaner system
    12. Nuclear fuel regeneration
    13. Pesticide manufacture
    14.Phosphoric acid manufacture
    15.Acid cleaning system
    16.Plate heat exchanger
    17. Selectivity filter system

    Specifications:

    bar/forging/ring

    AMS 5750

     

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy



  • Previous:
  • Next:

  • Write your message here and send it to us

    RELATED PRODUCTS