Nickel Alloy Incoloy 925 UNS N09925

\

Short Introduction:

HY 925/Incoloy 925/UNSN09925 is an age-hardenable alloy of nickel-chromium-iron. The additions of titanium and aluminum enable it to be age-hardened while molybdenum and copper contents enhance resistance to corrosive media. Designed primarily for applications in the production of gas.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    Y925 Material grades and equivalents

    HY 925 /UNSN09925

    HY 925 Chemical compostion:

    Alloy

    %

    Ni

    Cr

    Fe

    C

    Mn

    Si

    Cu

    S

    Al

    Ti

    P

    Mo

    HY 925

    Min.

    42

    19.5

    bal

    1.5

    0.15

    1.9

    2.5

    Max.

    46

    23.5

    0.03

    1

    0.5

    3

    0.03

    0.50

    2.4

    0.03

    3.5

    HY 925 Physical properties:

    Density

    8.14 g/cm3

    Melting point

    1343 ℃

    HY 925 minimum mechanical properties in the roomtemperature

    Alloy state

    Tensile strength
    Rm N/mm²

    Yield strength

    RP0.2 N/mm²

    Elongation

    A 5 %

    Solution treatment

    650

    300

    30

    HY 925 Characteristic as below

    This is an age-hardenable alloy of nickel-chromium-iron. The additions of titanium and aluminum enable it to be age-hardened while molybdenum and copper contents enhance resistance to corrosive media. Designed primarily for applications in the production of gas.

    HY 925 Application field

    It is used in the petroleum industry for applications such as gas well components, valves and tubing, as well as finding use in high-strength piping systems.

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy



  • Previous:
  • Next:

  • Write your message here and send it to us

    RELATED PRODUCTS

    WhatsApp Online Chat !