Nickel Alloy Inconel 601 UNS N06601

\

Short Introduction:

One of the mainly performance of HY601 / Inconel 601 / GB NS313 / UNS N06601/W.Nr.2.4851 NiCr23Fe / AFNOR NC23FeA is inexorability in high temperature, even in very inclement conditions. If in the process of heating and cooling cycle, 601 can generate the dense layer of oxide film to get high spalling resistance. 601 have good carbonation resistance. With excellent inoxidability in the high temperature of sulfur atmosphere since it has high chromium and aluminum content.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY 601 Material grades and equivalents

    Inconel 601 / GB NS313 / UNS N06601/W.Nr.2.4851 NiCr23Fe / AFNOR NC23FeA

    HY 601 Chemaical composition:

    Alloy

    %

    Ni

    Cr

    Fe

    C

    Mn

    Si

    Cu

    Al

    P

    S

    601

    Min.

    58

    21

    1.0

    Max.

    63

    25

    balance

    0.1

    1.5

    0.5

    1

    1.7

    0.02

    0.015

    HY 601 Physical properties

    Density

    8.1g/cm³

    Melting point

    1320-1370℃



    HY 601 Alloy m inimum mechanical properties in the room temperature

    Alloy state

    Tensile strength
    Rm N/mm²

    Yield strength
    R P0. 2N/mm²

    Elongation
    A 5 %

    Brinell hardness
    HB

    Annealing treatment

    650

    300

    30

    -

    Solution treatment

    600

    240

    30

    ≤220


    Characteristic as below

    1. Excellent inoxidability in the high temperature.
    2. Good resistance to carbonizing.
    3. Good inoxidabilitiy in sulfur atmosphere
    4.Good mechanical property in both room temperature and high temperature.
    5.Good resistance to stress corrosion cracking, 601 have high creep rupture strength since it limits the carbon content and grain size, so recommend to use for above 500℃ environment.

    HY 601 Metallurgical structure:
    601 is face-centered cubic lattice structure.

    HY 601 Corrosion resistance
    One of the mainly performance of 601 is inexorability in high temperature, even in very inclement conditions. If in the process of heating and cooling cycle, 601 can generate the dense layer of oxide film to get high spalling resistance. 601 have good carbonation resistance. With excellent inoxidability in the high temperature of sulfur atmosphere since it has high chromium and aluminum content.

    HY 601 Application field:
    1.The tray,basket and tool clamp in the heat treatment factory.
    2.Steel shares at annealing and radiation control, high-speed gas burners, Industrial furnace silk screen.
    3.Separate tank of ammonia reforming and catalytic support grid of nitric acid producing.
    4.Exhaust system parts
    5.Solid waste incinerator’s combustion chamber
    6.Channel support and soot dealing parts.
    7.Detoxification exhaust system components
    8.Oxygen re-heater

     

    Specifications

    Pipe Smls

    Pipe Welded

    Sheet/Plate

    Bar

    Forging

    Fitting

    Wire

    B167

    B517

    B168

    B166

    B564

    B366

    B166

     

     

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy





  • Previous:
  • Next:

  • Write your message here and send it to us

    RELATED PRODUCTS

    WhatsApp Online Chat !