Nickel cobalt base alloy AMS 5844 MP35N

\

Short Introduction:

MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties-ultra high strength, toughness, ductility and outstanding corrosion resistance.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY MP35N Material grades and equivalents

    MP35N/UNS R30035/ W.Nr 2.4999/ AMS 5844

    Introduction:

    HY MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties-ultra high strength, toughness, ductility and outstanding corrosion resistance. The alloy is work-strengthened and aged to obtain strength levels of 260 to 300 ksi(1793-2068 MPa). HY MP35N alloy resists corrosion in hydrogen sulfide, salt water and other chloride solution, as well as the mineral acids(nitric, hydrochloric, sulfuric).In addition, it has exceptional resistance to crevice and stress corrosion cracking in sea water and other hostile environments.

    Chemical composition:

    Weight%

    Ni

    Co

    Cr

    Mo

    Ti

    Fe

    Si

    Mn

    P

    B

    S

    C

    HY MP35N

    33

    Balance

    19

    9

    1

    1

    0.15

    0.15

    0.015

    0.01

    0.01

    0.03

    37

    21

    10.5

    Max

    Max

    Max

    Max

    Max

    Max

    Max

    Max

     Mechanical properties:

    MP35N Alloy

    Ultimate Tensile
    Strength

    0.2% Offset Yield
    Strength

    Elongation in
    4D

    Reduction of Area

    Hardness

    Shear
    Strength**

    Typical Properties
    of Solution Treated
    (Annealed)

    130 ksi(896 MPa)

    55 ksi(379 MPa)

    65%

    75%

    90 HRB

    Typical Properties
    of AMS 5844 Product after 4 Hour Age at 1050℉(556℃)*

    290 ksi(2000 MPa)

    280 ksi(1931 MPa)

    10%

    45%

    51 HRC

    AMS 5844 Specification Requirements after Aging 4 Hours at 1000-1200℉
    (538-648℃)

    260 ksi(1795 MPa),min.

    230 ksi(1585 MPa),min.

    8%,min.

    35%,min.

    150 ksi(1034 Mpa),min.

    The above data are longitudinal properties.

    *Tensile properties will change depending on product size.

    **Not required by AMS 5844, but this is guaranteed shear strength.

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

     

     




  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !