We thinks what customers think, the urgency of urgency to act in the interests of a customer position of principle, allowing for better quality, lower processing costs, prices are more reasonable, won the new and old customers the support and affirmation for OEM China High quality Pure nickel Alloy Nickel 201 UNS N02201 for Spain Manufacturer, We welcome new and old customers from all walks of life to contact us for future business relationships and mutual success!
Material grades and equivalents
Nickel 201 /N02201/ W.Nr 2.4061
HY N201Chemical composition
|
Alloy |
% |
Ni |
Fe |
C |
Mn |
Si |
Cu |
S |
|
HY N201 |
Min. |
Balance | ||||||
|
Max. |
0.4 |
0.02 |
0.35 |
0.35 |
0.25 |
0.01 |
HY N201Pysical properties
|
Density |
8.89 g/cm³ |
|
Melting point |
1440℃ |
HY N201 Alloy minimum mechanical properties in the room temperature
|
Product Form |
Condition |
Tensile strength |
Yield strength |
Elongation A5 % |
Brinell hardness |
|
Rod & Bar |
Hot Finished |
60-85 |
15-45 |
35-55 |
45-80 |
|
Rod & Bar |
Cold Drawn/Annealed or Hot-Finished/Annealed |
55-75 |
15-30 |
40-55 |
45-70 |
|
Plate |
Hot-Rolled/Annealed |
55-80 |
15-40 |
40-60 |
45-75 |
|
Sheet |
Annealed |
55-75 |
15-30 |
40-55 |
70 max |
|
Tube & Pipe |
Seamless Annealed |
55-75 |
12-30 |
40-60 |
70 max |
HY N201Characteristic as below:
Highly resistant to various reducing chemicals
Excellent resistance to caustic alkalies
High electrical conductivity
Excellent corrosion resistance to distilled and natural waters
Resistance to neutral and alkaline salt solutions
Excellent resistance to dry fluorine
Widely used to handle caustic soda
Good thermal, electrical and magnetostrictive properties
Offers some resistance to hydrochloric and sulfuric acids at modest temperatures and concentrations
HY N201 Application field :
Food processing equipment
Marine and offshore engineering
Salt production
Caustic handling equipment
Manufacture and handling of sodium hydroxide, particularly at temperatures above 300° F
Reactors and vessels in which fluorine is generated and reacted with hydrocarbons
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Provider foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,3rd Industrial District XiTou Village SongGang City Bao’An District ShenZhen Town GuangDong Province China
I am earning my own wedding day band from Inconel X-750 just to be diverse. The material is a agony to do the job with thanks to the superior nickel/chromium articles. The lathe is a LeBlond “dual generate” with an Aloris-copy device article. I built an adapter for the one.25″ boring bar socket to sleeve it down to a 5/8″ side-lock drill shank. I utilised an indicator to sweep the device holder, inserting it instantly on center. The drill is a Seco CrownLoc As well as with .625″ tip, running at around 80sfm, hand feed with plenty of stress, and drenched in reducing oil (not demonstrated in pic). Chips had been astonishingly limited of course, I had to withdrawal the device numerous moments to eliminate chips, due to the fact they weren’t becoming flushed by coolant.