Online Exporter Nickel Alloy Inconel 601 UNS N06601 Manufacturer in South Korea
To constantly improve the management system by virtue of the rule of "sincerely, good faith and quality are the base of enterprise development", we widely absorb the essence of related products internationally, and constantly develop new products to meet the demands of customers for Online Exporter Nickel Alloy Inconel 601 UNS N06601 Manufacturer in South Korea, If you are interested in our products, please feel free to send us your inquiry. We sincerely hope to establish win-win business relationships with you.
HY 601 Material grades and equivalents
Inconel 601 / GB NS313 / UNS N06601/W.Nr.2.4851 NiCr23Fe / AFNOR NC23FeA
HY 601 Chemaical composition:
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Cu |
Al |
P |
S |
601 |
Min. |
58 |
21 |
1.0 |
|||||||
Max. |
63 |
25 |
balance |
0.1 |
1.5 |
0.5 |
1 |
1.7 |
0.02 |
0.015 |
HY 601 Physical properties
Density |
8.1g/cm3 |
Melting point |
1320-1370℃ |
HY 601 Alloy m inimum mechanical properties in the room temperature
Alloy state |
Tensile strength |
Yield strength |
Elongation |
Brinell hardness |
Annealing treatment |
650 |
300 |
30 |
- |
Solution treatment |
600 |
240 |
30 |
≤220 |
Characteristic as below:
1. Excellent inoxidability in the high temperature.
2. Good resistance to carbonizing.
3. Good inoxidabilitiy in sulfur atmosphere
4.Good mechanical property in both room temperature and high temperature.
5.Good resistance to stress corrosion cracking, 601 have high creep rupture strength since it limits the carbon content and grain size, so recommend to use for above 500℃ environment.
HY 601 Metallurgical structure:
601 is face-centered cubic lattice structure.
HY 601 Corrosion resistance
One of the mainly performance of 601 is inexorability in high temperature, even in very inclement conditions. If in the process of heating and cooling cycle, 601 can generate the dense layer of oxide film to get high spalling resistance. 601 have good carbonation resistance. With excellent inoxidability in the high temperature of sulfur atmosphere since it has high chromium and aluminum content.
HY 601 Application field:
1.The tray,basket and tool clamp in the heat treatment factory.
2.Steel shares at annealing and radiation control, high-speed gas burners, Industrial furnace silk screen.
3.Separate tank of ammonia reforming and catalytic support grid of nitric acid producing.
4.Exhaust system parts
5.Solid waste incinerator’s combustion chamber
6.Channel support and soot dealing parts.
7.Detoxification exhaust system components
8.Oxygen re-heater
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Check out additional TIG Welding Video clips from Weld.com:
http://www.weld.com/index.php/Mr-Tig-Blog/
Subscribe on YouTube and Never ever Miss a Video!
http://www.youtube.com/channel/UCM0kHJXSHR1k1wtLuliKmHg?sub_confirmation=one
Pay a visit to the Welding Discussion board to Carry on the Dialogue and Compete in Month to month Contests!
http://www.weld.com/index.php/Weekend-Warrior-Welding-Discussion board/groups.html
Fb: https://www.fb.com/WeldDotCom
Twitter: https://twitter.com/WeldDotCom
—————————————————————————–
Weld.com welding films are a collection of welding displays that are loaded with welding strategies, tricks and hints that will support you drop that perfect bead each individual time! Whether you are making an attempt to become far better in the locations of TIG Welding, MIG Welding, Adhere Welding or Slicing Weld.com has what you will need. All films are shot from “guiding the hood” so you can get the welders standpoint. In addition to exhibiting you how to weld, many periods we will clearly show you popular issues and how to steer clear of them.
New episodes each individual Friday!
Early launch on the discussion board!
I am earning my own wedding day band from Inconel X-750 just to be diverse. The material is a agony to do the job with thanks to the superior nickel/chromium articles. The lathe is a LeBlond “dual generate” with an Aloris-copy device article. I built an adapter for the one.25″ boring bar socket to sleeve it down to a 5/8″ side-lock drill shank. I utilised an indicator to sweep the device holder, inserting it instantly on center. The drill is a Seco CrownLoc As well as with .625″ tip, running at around 80sfm, hand feed with plenty of stress, and drenched in reducing oil (not demonstrated in pic). Chips had been astonishingly limited of course, I had to withdrawal the device numerous moments to eliminate chips, due to the fact they weren’t becoming flushed by coolant.