Trademark | GB | AISI/ASTM | UNS | W.Nr | BS | AFNOR | JIS | ID | |
Inconel Alloys |
Inconel 600 | GB NS312 | UNS N06600 | W.Nr 2.4816 | BS NA14 | AFNOR NC15FE | JIS NCF600 | ||
Inconel 601 | GB NS313 | UNS N06601 | W.Nr 2.4851 | AFNOR NC23FeA | |||||
Inconel 617 | UNS N06617 | W.Nr 2.4663 | AFNOR NC22KDA | ||||||
Inconel 625 | GB NS336 | UNS N06625 | W.Nr 2.4856 | BS NA21 | AFNOR NC22DNB | JIS NCF625 | |||
Inconel 686 | UNS N06686 | W.Nr 2.4606 | |||||||
Inconel 690 | GB NS315 | UNS N06690 | AFNOR NC30Fe | ||||||
Inconel 718 | GB GH4169 | UNS N07718 | W.Nr 2.4668 | BS NA51 | AFNOR NC19FeNb | ||||
Inconel 725 | UNS N07725 | ||||||||
Inconel 783 | UNS R30783 | ||||||||
Inconel X-750 | GB GH4145 | UNS N07750 | W.Nr 2.4669 | AFNOR NC15FeT | JIS NCF750B | ||||
Incoloy Alloys |
Incoloy 800 | GB NS111 | UNS N08800 | W.Nr 1.4876 | BS NA15 | AFNOR Z8NC32.21 | JIS NCF800B /JIS NCE2B |
||
Incoloy 800H | GB NS112 | UNS NO8810 | W.Nr 1.4958 | BS NA15 (H) | AFNOR Z8NC33.21 | ||||
Incoloy 800HT | UNS N08811 | W.Nr 1.4959 | BS NA15 (HT) | ||||||
Incoloy 825 | GB NS142 | UNS N08825 | W.Nr 2.4858 | BS NA16 | AFNOR NC21FeDu | JIS NCF825 | |||
Incoloy 901 | UNS N09901 | W.Nr 2.466 | |||||||
Incoloy 925 | UNS N09925 | ||||||||
Incoloy 926 | UNS N08926 | W.Nr 1.4529 | AFNOR X1NiCrMoCu | ||||||
Incoloy A-286 | GB GH2132 | UNS S66286 | W.Nr 1.498 | AFNOR ZbNCT25 | JIS SUH660 | ||||
Hastelloy Alloys |
Hastelloy B | GB NS321 | UNS N10001 | ||||||
Hastelloy B-2 | GB NS322 | UNS N10665 | W.Nr 2.4617 | AFNOR NiMo28 | |||||
Hastelloy C | GB NS333/GB NS3303 | UNS N06003 | W.Nr 2.4819 | BS NA45 | |||||
Hastelloy C4 | UNS N06455 | AFNOR NC16D16M | |||||||
Hastelloy C-22 | UNS N06022 | W.Nr 2.4602 | AFNOR NU-30M | ||||||
Hastelloy C276 | GB NS334 | UNS N10276 | W.Nr 2.4819 | BS NC17D | AFNOR NiMo16Cr15 | ||||
Hastelloy X | GB GH3536/GB GH536 | UNS N06002 | W.Nr 2.4665 | AFNOR NC22FeD | |||||
Monel Alloys |
Monel 400 | UNS N04400 | W.Nr 2.436 | BS NA 12 | AFNOR Nu 30 | ||||
Monel K-500 | UNS N05500 | AFNOR Nu30AT | |||||||
Nickel Alloys |
Nickel 200 | UNS N02200 | W.Nr 2.406 | AFNOR Ni01/AFNOR N-100M | |||||
Nickel 201 | UNS N02201 | W.Nr 2.4061 | AFNOR Ni02 | ||||||
Nimonic Alloys |
Nimonic 75 | UNS N06075 | W.Nr 2.4951 &W.Nr 2.4630 | AFNOR NC20T | |||||
Nimonic 80A | UNS N07080 | W.Nr 2.4952 | AFNOR NC20TA | ||||||
Nimonic 90 | UNS N09901 | W.Nr 2.4662 | |||||||
Cobalt Alloys |
MP35N | AMS 5844 | UNS R30035 | W.Nr 2.4999 | |||||
Refractaloy 26 | UNS R30188 | ||||||||
Stellite 6 | ASTM 5387C-2001 | UNS R3006 | |||||||
Nickel 201 | |||||||||
Alloy L605 | UNS R30605 | ||||||||
Haynes 188 | GB GH5188 | UNS R30188 | W.Nr 2.4683 | ||||||
Waspaloy Alloy | GB GH4738 | UNS N07001 | W.Nr 2.4654 | ||||||
Iron Alloys |
ASTM Alloy31 | UNS N08031 | W.Nr 1.4562 | ||||||
Invar 36 | GB 4J36 | UNS K93600 | W.Nr 1.3912 | BS X1NiCrMoCu | AFNOR Fe-Ni36 | ||||
GB 4J29 | ASTM F15 | W.Nr 1.981 | JIS EMAS-1001 | ||||||
Nickel 201 | |||||||||
GB 1J50 | JIS PB | ||||||||
GB 3J53 | |||||||||
GB 1J79 | ASTM Alloy4 | ||||||||
Nitronic 50 | ASTM XM-19 | UNS S20910 | ID Fxm-19 | ||||||
Nitronic 60 | ASTM Alloy218 | UNS S21800 | |||||||
GB 05Cr17Ni4Cu4Nb | ASTM 630/ASTM 17-4PH | UNS S17400 | W.Nr 1.4507 | JIS SUS630 | |||||