Our company insists all along the quality policy of "product quality is base of enterprise survival; customer satisfaction is the staring point and ending of an enterprise; persistent improvement is eternal pursuit of staff" and the consistent purpose of "reputation first, customer first" for Professional High Quality Iron alloy Stainless Steel 17-4PH to Mali Factories, We welcome customers, business associations and friends from all parts of the world to contact us and seek cooperation for mutual benefits.
HY 17-4PH Material grades and equivalents |
|
||
UNS |
AISI/ASTM |
JIS |
W.Nr |
S17400 |
630,17-4PH |
SUS630 |
1.4542 |
HY 17-4PH Chemical composition: |
|
|
|
|
|
|
|
|
|||
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
S |
Cu |
Nb |
P |
HY 17-4PH |
Min. |
3 |
15.5 |
balance |
|
|
|
|
3 |
0.15 |
|
Max. |
5 |
17.5 |
0.07 |
1 |
1 |
0.03 |
5 |
0.45 |
0.035 |
HY 17-4PH Physical properties |
||
Density |
7.78/cm3 |
|
Melting point |
1400-1440 °C |
|
HY 17-4PH Minimum mechanical properties in the room temperature |
||||||
Status |
Tensile strength |
Yield strength |
Elongation |
HRC(HBS) |
|
|
Rm N/mm² |
Rp0.2 N/mm² |
A5 % |
|
|
||
480°C age |
≥1310 |
≥1180 |
≥10 |
≥40 |
|
|
550°C Age |
≥1060 |
≥1000 |
≥12 |
≥35 |
|
|
580°C age |
≥1000 |
≥865 |
≥13 |
≥31 |
|
|
620°C age |
≥930 |
≥325 |
≥16 |
≥28 |
|
|
HY 17-4PH Characteristic: |
|
|
|
|
|
||
High strength and hardness, good welding performance and corrosion resistance |
|||||||
|
|
|
|
|
|
|
|
HY 17-4PH Application range and field: |
|
|
|
|
|||
Used in components with high strength and corroson resistance |
|
Regular shape for all kinds of alloys |
|||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Inconel – Nickel Dependent Super Alloy – 600, 625, 718, X-750 Qualities and Programs August 2013 Inconel is a tremendous alloy and mixes effectively with Copper. Inconel arrives in a lot of varieties: Round Bar, Plate, Sheet, Pipe, Tube. Inconel is hard to machine for the reason that it perform hardens, Inconel 625 can be welded a bit.
High successful HRSA turbine blade roughing on Starrag LX 051
- Materials technical specs: Nimonic 80A, NiCr20TiAl (2.4952)
- MMR: sixteen.nine cm3/min