Pure nickel Alloy Nickel 201 UNS N02201

\

Short Introduction:

HY N201/Nickel 201/N02201/W.Nr 2.4061 has highly resistant to various reducing chemicals,excellent resistance to caustic alkalies,high electrical conductivity


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    Material grades and equivalents

    Nickel 201 /N02201/ W.Nr 2.4061

    HY N201Chemical composition

    Alloy

    %

    Ni

    Fe

    C

    Mn

    Si

    Cu

    S

    HY N201

    Min.

    Balance

    Max.

    0.4

    0.02

    0.35

    0.35

    0.25

    0.01

    HY N201Pysical properties

    Density

    8.89 g/cm³

    Melting point

    1440℃

    HY N201 Alloy minimum mechanical properties in the room temperature

    Product Form

    Condition

    Tensile strength
    Rm N/mm²

    Yield strength
    RP0.2 N/mm²

    Elongation

    A5 %

    Brinell hardness
    HB

    Rod & Bar

    Hot Finished

    60-85

    15-45

    35-55

    45-80

    Rod & Bar

    Cold Drawn/Annealed or Hot-Finished/Annealed

    55-75

    15-30

    40-55

    45-70

    Plate

    Hot-Rolled/Annealed

    55-80

    15-40

    40-60

    45-75

    Sheet

    Annealed

    55-75

    15-30

    40-55

    70 max

    Tube & Pipe

    Seamless Annealed

    55-75

    12-30

    40-60

    70 max

    HY N201Characteristic as below:

    Highly resistant to various reducing chemicals

    Excellent resistance to caustic alkalies

    High electrical conductivity

    Excellent corrosion resistance to distilled and natural waters

    Resistance to neutral and alkaline salt solutions

    Excellent resistance to dry fluorine

    Widely used to handle caustic soda

    Good thermal, electrical and magnetostrictive properties

    Offers some resistance to hydrochloric and sulfuric acids at modest temperatures and concentrations

    HY N201 Application field

    Food processing equipment

    Marine and offshore engineering

    Salt production

    Caustic handling equipment

    Manufacture and handling of sodium hydroxide, particularly at temperatures above 300° F

    Reactors and vessels in which fluorine is generated and reacted with hydrocarbons

     

    Specification

    Pipe Smls

    Pipe Welded

    Sheet/Plate

    Bar

    Fitting

    B161

    B622

    B162

    B160

    B163

     

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy