We are ready to share our knowledge of marketing worldwide and recommend you suitable products at most competitive prices. So Profi Tools offer you best value of money and we are ready to develop together with Special Design for Nickel Alloy Nimonic 80A UNS N07080 Factory in Bulgaria, We cordially welcome customers from at home and abroad to join us and cooperate with us to enjoy a better future.
HY 80A Material grades and equivalents
Nimonic 80A /UNS N07080 / SEW VDIUV W. Nr. 2.4952 / AFNOR NC20TA
HY N80A Chemaical composition:
Alloy |
% |
Ni |
Cr |
Fe |
Mn |
Si |
P |
S |
Al |
Ti |
C |
Co |
B |
Zr |
Cu |
80A |
Min. |
Balance |
18 |
1.0 |
1.8 |
||||||||||
Max. |
21 |
3.0 |
1.0 |
1.0 |
0.02 |
0.015 |
1.8 |
2.7 |
0.1 |
2.0 |
0.008 |
0.15 |
0.2 |
HY N80A Physical properties:
Density |
8.19 g/cm3 |
Melting point |
1320-1365℃ |
HY N80 A minimum mechanical properties in the room temperature :
Status |
Tensile strength |
Yield strength |
Elongation |
HY N80A |
930 |
620 |
20 |
Characteristic as below:
A nickel-chromium alloy similar to NIMONIC alloy 75 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good corrosion and oxidation resistance and high tensile and creep-rupture properties at temperatures to 1500°F (815°C).
Used for gas-turbine components (blades, rings, and discs), bolts, tube supports in nuclear steam generators, die-casting inserts and cores, and exhaust valves in internal-combustion engines.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Melting down 1 gram bars of Silver, Copper, Nickel and Brass with hydrogen and oxygen. Brass is previously an alloy of copper and zinc, and did not soften down effortless as a I figured out from my Brass, Guide and Gunpowder video clip. I then blend the a few workable metals Silver, copper and nickel to generate…….Silvcopickel
SUBSCRIBE: http://comprehensive.sc/1bnslc9
Facebook: http://comprehensive.sc/1dT2aaM
RHNB Vs. Watermelon – http://comprehensive.sc/1bns60F
RHNB Vs. Jello – http://comprehensive.s/1bns0WF RHNB Vs. Elmers Glue – http://comprehensive.sc/1dT1TEM
RHNB Entire Playlist – http://comprehensive.sc/1dT1WjP -Want to ship an object / materials / substance to be RHNB’d or HHO’d? Send Here with a comprehensive credit of your donation! PO Box 21 96 Seymour St. Tonawanda NY 14150 Usa
Visit my site for additional Recommendations, Films, Do it yourself assignments and additional:
http://www.mjlorton.com/
—————————–Click “Display additional”—————————————
A information on making use of the correct applications to crimp connectors, strip wire and implement warmth shrink.
You should guidance my information generation by making use of my Amazon Retail store:
http://astore.amazon.com/m0711-twenty
Purchase these applications and connectors below: http://astore.amazon.com/m0711-twenty?node=ten&site=one
——————— Click “Display additional” ——————————-
My site and forum:- http://www.mjlorton.com
Donations and contributions:- http://www.mjlorton.com
My techie channel MJLorton – Solar Power and Digital Measurement Products – http://www.youtube.com/MJLorton
My Techie Amazon Retail store: http://astore.amazon.com/m0711-twenty
My other channel VBlogMag – For nearly any matter beneath the sun! – http://www.youtube.com/VBlogMag
My VBlogMag Amazon Retail store: http://astore.amazon.com/vblogmag-twenty
———————————————————————–
=================================================
Online video sponsor, Pass Ltd – their internet websites:
http://www.tester.co.united kingdom/?cmid=QmhzQjcxYjVlc1E9&afid=bFcwbzliNzVDc289&ats=K2EyUjZNTDh3UTA9 – Examination Products and Examination-meter suppliers and
http://www.calibrate.co.united kingdom/?cmid=QmhzQjcxYjVlc1E9&afid=bFcwbzliNzVDc289&ats=S3Yxd2tOMjVISzA9 – Calibration and support of exam tools
=================================================
Additional dialogue and link to NASA information below:
http://mjlorton.com/forum/index.php?matter=244.
In this online video:
* Deciding upon the correct wire gauge (AWG – American Wire Gauge) for the crimp connector.
* Employing the correct applications to strip the insulation from the wire.
* The correct way to insert the wire into the crimp connector
* Employing the correct crimp applications to crimp the connector
* How to implement warmth shrink accurately to the wire and crimp connector.