We have a highly efficient team to deal with inquiries from customers. Our goal is "100% customer satisfaction by our product quality, price & our team service" and enjoy a good reputation among clients. With many factories, we can provide a wide range of Trending Products Nickel Alloy Nimonic 90 UNS N09901 for Guatemala Importers, We sincerely welcome all guests to set up business relationships with us on the basis of mutual benefits. Please contact us now. You will get our professional reply within 8 hours.
HY N90 Material grades and equivalents
Nimonic 90/GB GH90/ UNS N07090 / BS Nimonic90/ W. Nr. 2.4632
HY N90 characteristics and application fields of summary:
This alloy is aging strengthen ni-based deformation high temperature ally, with a high amount of cobalt and many kinds of strengthening element, this alloy in 815 ~ 870 °C have high tensile strength and contravariance ability, good oxidation resistance and corrosion resistance, cold and heat alternately repeatedly in under the action of a higher fatigue strength and good formability and weldability. Used for turbine engine turbine dish, leaf, high temperature fasteners, card hoop, seals and elastic components etc.
HY N90 chemical ingredients: (GB/T14992-2005)
Alloy | % | Ni | Cr | Fe | Zr | B | Co | C | Mn | Si | S | Cu | Al | Ti |
HY N90 | Min | Bal | 18.0 | 15.0 | 1.0 | 2.0 | ||||||||
Max | 21.0 | 1.5 | 0.15 | 0.02 | 21.0 | 0.13 | 0.4 | 0.8 | 0.015 | 0.2 | 2.0 | 3.0 |
HY N90 physical ability:
density g/cm3 |
M.point °C |
Heat transfer Rate λ/(W/m•°C) |
specific heat capacity J/kg•°C |
modulus of elasticityGPa | shear elasticityGPa | R μΩ•m |
coefficient of linear expansion a/10-6°C-1 |
|
8.2 | 1400 | 21.76(100°C) | 225 | 12.7(20~100°C) |
HY N90 force ablity:
Heat treatment | Tensile Strength σb/MPa | Yield Strength σp0.2/MPa | Elongationσ5 /% | HB HBS |
Solution treatment | 820 | 590 | 8 |
Nimonic90 process performance and requirements:
1, the alloy in forging easily produce inside crack, allow hammer blow, don’t allow low temperature chamfering. Ingot outfit furnace temperature is not higher than 700 °C, 1150 °C ± final heating temperature 10 °C, open forging not below 1060 °C temperature, and forging temperature not less than 950 °C.
2, the size of the average grain degrees of alloy forgings and deformation degree, eventually forging is closely related to the temperature.
3, alloy in solid solution state can be inert gas protection electric arc welding and tungsten very flash butt weld.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Check out additional TIG Welding Video clips from Weld.com:
http://www.weld.com/index.php/Mr-Tig-Blog/
Subscribe on YouTube and Never ever Miss a Video!
http://www.youtube.com/channel/UCM0kHJXSHR1k1wtLuliKmHg?sub_confirmation=one
Pay a visit to the Welding Discussion board to Carry on the Dialogue and Compete in Month to month Contests!
http://www.weld.com/index.php/Weekend-Warrior-Welding-Discussion board/groups.html
Fb: https://www.fb.com/WeldDotCom
Twitter: https://twitter.com/WeldDotCom
—————————————————————————–
Weld.com welding films are a collection of welding displays that are loaded with welding strategies, tricks and hints that will support you drop that perfect bead each individual time! Whether you are making an attempt to become far better in the locations of TIG Welding, MIG Welding, Adhere Welding or Slicing Weld.com has what you will need. All films are shot from “guiding the hood” so you can get the welders standpoint. In addition to exhibiting you how to weld, many periods we will clearly show you popular issues and how to steer clear of them.
New episodes each individual Friday!
Early launch on the discussion board!
NEW 2016 Chrysler three hundred S Alloy Edition Sedan with a Gloss Black Paint finish. AWD that seats five with a three.two L V-six engine and an eight velocity computerized transmission. 19″ alluminum alloy rims with Michelin Primacy MXM4 tires. This sedan will come thoroughly loaded with keyless entry, distant get started, power locks, home windows, mirrors, Beats by Dre audio system, AM/FM, Sirius Sat radio, Lcd display screen in the entrance with back up digicam, leather all over with heated entrance and rear seats and so significantly a lot more. Come check out it out at Ponoka Chrysler and see what else it has to present, we are located on the south conclusion of Ponoka just off of HWY 2A.
Stock# 16C37644
Sarah Johnson,
Ponoka Chrysler
6510 39th Ave Ponoka, AB T4J 1J8
Toll Cost-free: 1(800) 265-6851
Cellphone: (403) 783-5383
Fax: (403) 783-8140
E-mail: sjohnson@ponokachrysler.com
Like us on Fb- https://www.facebook.com/PonokaChrysler/
Abide by us on Instargram- https://www.instagram.com/ponokadodge/
Abide by us on Twitter- https://twitter.com/PonokaDodgeRam
Abide by us on Pintrest- https://www.pinterest.com/ponokachrysler/