Well-designed Heat Resistant Wire Cr30Ni70 Nichrome alloy wire for Mauritius Manufacturers
We are ready to share our knowledge of marketing worldwide and recommend you suitable products at most competitive prices. So Profi Tools offer you best value of money and we are ready to develop together with Well-designed Heat Resistant Wire Cr30Ni70 Nichrome alloy wire for Mauritius Manufacturers, Please send us your specifications and requirements, or feel free to contact us with any questions or inquiries that you may have.
HY 3070 Material grades and equivalents
Cr30Ni70 / Ni70Cr30
HY 3070 Grade property performance
|
Grade property performance |
HY 3070 |
|
|
% Main Chemical Composition |
Ni |
Balance |
|
Cr |
28.0-31.0 |
|
|
Fe |
≤1.0 |
|
|
℃ Max contimnous service Temp. of element |
1200 |
|
|
Resistiuity |
1.09 |
|
|
g/cm3 Density |
8.4 |
|
|
KJ/M.h℃ Thermal conductivity |
60.3 |
|
|
Coefficient of linear expansion |
18 |
|
|
Melting point≈ ℃ (approxi) |
1400 |
|
|
% Elongation |
≥20 |
|
|
Micrograhic structure |
austenite |
|
|
Magnetic property |
nonmagnetic |
|
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Welding Inconel 718
http://www.weldingtipsandtricks.com/metals-and-how-to-weld-nickel.html