The company keeps to the operation concept "scientific management, high quality and efficiency primacy, customer supreme for Wholesale 100% Original Nickel Alloy Inconel 625 UNS N06625 in Venezuela, Competitive price with high quality and satisfying service make us earned more customers.we wish to work with you and seek common development.
HY 625 Material grades and equivalents
Inconel 625/ GB NS336 / UNS N06625/ SEW VDIUV W.Nr.2.4856 NiCr22Mo9Nb / BS NA 12 / AFNOR NC22DNB
HY 625 Chemical composition
Alloy |
% |
Ni |
Cr |
Mo |
Nb+N |
Fe |
Al |
Ti |
C |
Mn |
Si |
Cu |
P |
S |
625 |
Min. |
58 |
20 |
8 |
3.15 |
|||||||||
Max. |
23 |
10 |
4.15 |
5 |
0.4 |
0.4 |
0.1 |
0.5 |
0.5 |
0.5 |
0.015 |
0.015 |
HY 625 Pysical properties
Density |
8.4 g/cm3 |
Melting point |
1290-1350°C |
HY 625 Alloy m inimum mechanical properties in the room temperature
Alloy state |
Tensile strength |
Yield strength |
Elongation A 5 % |
Brinell hardness |
625 |
760 |
345 |
30 |
≤220 |
Characteristic as below
1. Excellent corrosion resistance of different kinds of media in both oxidation and reduction environments.
2. Excellent resistance of pitting and crevice corrosion, and won’t happen stress corrosion cracking because of chloride.
3.Excellent resistance of the inorganic acid corrosion performance, such as nitric acid, phosphoric acid, sulfuric acid, hydrochloric acid and the mixture of sulfuric acid and hydrochloric acid.
4. Excellent corrosion resistance of different kinds of inorganic acid mixture performance.
5. Good corrosion resistance of a variety of concentrations of hydrochloric acid when the temperature up to 40°C .
6. Good machining and welding, no weld cracking sensitivity.
7. Have pressure vessel authentication for the wall temperature between -196 ~ 450°C .
8. Apply for the highest standard lever VII of acidic environment by the NACE ( MR-01-75) authorized.
HY 625 Corrosion resistance
625 own a very good corrosion resistance in many media, especially with excellent resistance to pitting, crevice corrosion, intercrystalline corrosion, and erode in oxide, also good resistance to inorganic acid corrosion, such as nitric acid, phosphoric acid, sulfuric acid and hydrochloric acid. 625 can resist the alkali and organic acid corrosion in the oxidation and reduction environment. Effect resists the chloride reduction stress corrosion cracking. Normally no corrosion in the sea-water and industry environments since high corrosion resistance to the sea-water and salting liquid,as well as in high temperature, without sensitivity during welding. 625 have the resistance to oxidation and carbonizing in the static and cycle environments, also hacve the resistance the chlorine corrosion.
HY 625 Application field
Soften annealing low carbon alloy 625 widely used in the chemical process industry, good corrosion resistance and high strength made it an good choice for structural parts. 625 have application in sea-water for local mechanical stress attach.
HY 625 Typical application field as below
1 .The Organic chemical process parts contains chloride, especially in the use of acid chloride catalyst.
2. The digester and bleacherin the use of paper pulp and paper making industry.
3.Absorption tower, re-heater,gas import board, fan, blender, fair water fin, flue and so on for using in flue gas desulfurization system.
4. The equipment and parts in the use of acidic gas environments.
5. Acetic acid and anhydride reaction generator
6. Sulfur acid cooling
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Visit my site for additional Recommendations, Films, Do it yourself assignments and additional:
http://www.mjlorton.com/
—————————–Click “Display additional”—————————————
A information on making use of the correct applications to crimp connectors, strip wire and implement warmth shrink.
You should guidance my information generation by making use of my Amazon Retail store:
http://astore.amazon.com/m0711-twenty
Purchase these applications and connectors below: http://astore.amazon.com/m0711-twenty?node=ten&site=one
——————— Click “Display additional” ——————————-
My site and forum:- http://www.mjlorton.com
Donations and contributions:- http://www.mjlorton.com
My techie channel MJLorton – Solar Power and Digital Measurement Products – http://www.youtube.com/MJLorton
My Techie Amazon Retail store: http://astore.amazon.com/m0711-twenty
My other channel VBlogMag – For nearly any matter beneath the sun! – http://www.youtube.com/VBlogMag
My VBlogMag Amazon Retail store: http://astore.amazon.com/vblogmag-twenty
———————————————————————–
=================================================
Online video sponsor, Pass Ltd – their internet websites:
http://www.tester.co.united kingdom/?cmid=QmhzQjcxYjVlc1E9&afid=bFcwbzliNzVDc289&ats=K2EyUjZNTDh3UTA9 – Examination Products and Examination-meter suppliers and
http://www.calibrate.co.united kingdom/?cmid=QmhzQjcxYjVlc1E9&afid=bFcwbzliNzVDc289&ats=S3Yxd2tOMjVISzA9 – Calibration and support of exam tools
=================================================
Additional dialogue and link to NASA information below:
http://mjlorton.com/forum/index.php?matter=244.
In this online video:
* Deciding upon the correct wire gauge (AWG – American Wire Gauge) for the crimp connector.
* Employing the correct applications to strip the insulation from the wire.
* The correct way to insert the wire into the crimp connector
* Employing the correct crimp applications to crimp the connector
* How to implement warmth shrink accurately to the wire and crimp connector.
Metals playlist: https://www.youtube.com/playlist?record=PL64F10A579EB0A526
far more at http://scitech.quickfound.net/
Aluminum creation system like mining bauxite in Arkansas and Jamaica, transport Jamaican ore from Ocho Rios, reduction of the bauxite at vegetation in the US., and manufacturing of aluminum ingots and forming aluminum sheets and personalized parts. Animated intro is equivalent to present-day Fortunate Strike and Rheingold beer commercials.
“How aluminum contributes to everyday dwelling and national protection: appliances, packaging, airplanes, and so on. With fantastic quit-movement animation.”
Reupload of a previously uploaded film with enhanced online video & audio.
Public domain film from the Library of Congress Prelinger Archives, slightly cropped to take out uneven edges, with the component ratio corrected, and a single-move brightness-distinction-coloration correction & delicate online video noise reduction utilized.
The soundtrack was also processed with volume normalization, noise reduction, clipping reduction, and/or equalization (the resulting audio, while not ideal, is much significantly less noisy than the unique).
http://creativecommons.org/licenses/b…
http://en.wikipedia.org/wiki/Aluminium
Aluminium… is a silvery white member of the boron team of chemical aspects. It has the symbol Al, and its atomic variety is thirteen. It is not soluble in h2o beneath typical instances. Aluminium is the 3rd most considerable element (right after oxygen and silicon), and the most considerable steel, in the Earth’s crust. It would make up about 8% by bodyweight of the Earth’s sound floor. Aluminium steel is much too reactive chemically to manifest natively. As an alternative, it is discovered put together in more than 270 distinct minerals. The chief ore of aluminium is bauxite.
Aluminium is impressive for the metal’s very low density and for its skill to resist corrosion due to the phenomenon of passivation. Structural factors produced from aluminium and its alloys are vital to the aerospace sector and are significant in other places of transportation and structural resources. The most helpful compounds of aluminium, at least on a bodyweight foundation, are the oxides and sulfates…
Bodily
Aluminium is a soft, resilient, light-weight, ductile and malleable steel with appearance ranging from silvery to boring gray, relying on the floor roughness. Aluminium is nonmagnetic and does not simply ignite. A fresh film of aluminium film serves as a excellent reflector (around 92%) of noticeable light and an outstanding reflector (as much as 98%) of medium and much infrared radiation. The generate strength of pure aluminium is seven–11 MPa, even though aluminium alloys have generate strengths ranging from two hundred MPa to 600 MPa. Aluminium has about a single-3rd the density and stiffness of metal. It is simply machined, solid, drawn and extruded.
Corrosion resistance can be outstanding due to a slender floor layer of aluminium oxide that varieties when the steel is exposed to air, proficiently protecting against further oxidation. The strongest aluminium alloys are significantly less corrosion resistant due to galvanic reactions with alloyed copper. This corrosion resistance is also usually drastically decreased when lots of aqueous salts are current, specially in the presence of dissimilar metals…
Aluminium mirror end has the best reflectance of any steel in the two hundred–400 nm (UV) and the 3,000–10,000 nm (much IR) locations in the 400–seven hundred nm noticeable selection it is slightly outperformed by tin and silver and in the seven hundred–3000 (near IR) by silver, gold, and copper.
Aluminium is a excellent thermal and electrical conductor, possessing 59% the conductivity of copper, both of those thermal and electrical…
Aluminium varieties powerful chemical bonds with oxygen. In contrast to most other metals, it is tough to extract from ore, these kinds of as bauxite, due to the vitality essential to minimize aluminium oxide (Al2O3)…
Aluminium electrolysis with the Hall-Héroult system consumes a large amount of vitality, but substitute procedures ended up generally discovered to be significantly less feasible economically and/or ecologically…
In 2005, the People’s Republic of China was the leading producer of aluminium with pretty much a a single-fifth earth share, followed by Russia, Canada, and the Usa, experiences the British Geological Study…
http://en.wikipedia.org/wiki/Reynolds…
The Reynolds Metals Company was founded in 1919 as the U.S. Foil Company in Louisville, Kentucky by Richard S. Reynolds, Sr., a nephew of tobacco king R. J. Reynolds. To begin with, the new organization equipped guide and tin foil wrappers to cigarette and candy firms. In 1924, the U.S. Foil bought the maker of Eskimo Pies, which ended up wrapped in foil. In 1928, Reynolds bought Robertshaw Thermostat, Fulton Sylphon, and portion of Beechnut Foil, introducing them to U.S. Foil to make Reynolds Metals…
The organization started creating aluminum foil for packaging in 1926.