Wholesale Price Nickel Alloy Hastelloy X UNS N06002 for Slovakia Manufacturers
We keep improving and perfecting our products and service. At the same time, we work actively to do research and development for Wholesale Price Nickel Alloy Hastelloy X UNS N06002 for Slovakia Manufacturers, If you have any comments about our company or products, please feel free to contact us, your coming mail will be highly appreciated.
HY HX Material grades and equivalents
Hastelloy X / GB GH3536&GH536/UNS N06002 / SEW VDIUV W.Nr.2.4613 / AFNOR NC22FeD
HY HX | ||||||||||||||||
UNS | Trademark | W.Nr | ||||||||||||||
N06002 | HY HX | 2.4613 | ||||||||||||||
HY HX Chemical compostion: | ||||||||||||||||
Alloy | % | Ni | Cr | Fe | C | Mn | Si | Cu | S | B | Ti | P | Co | W | Mo | Al |
HY HX | Min. | balance | 20.5 | 17 | 0.05 | 0.5 | 0.2 | 8 | ||||||||
Max. | 23 | 20 | 0.15 | 1 | 1 | 0.5 | 0.015 | 0.01 | 0.15 | 0.025 | 2.5 | 1 | 10 | 0.5 | ||
HY HX Physical properties: | ||||||||||||||||
Density | 8.28 g/cm3 | |||||||||||||||
Melting Point | 1295-1381 ℃ |
Hastelloy X Characteristic:
Good oxidation and corrosion resistance. Below 900 °C with middle elevated temperature stress rupture and creep rupture strength; good formability with cold working and hot working and excellent welding fabrication.
Hastelloy X Applied field:
Aero-engine combustion chamber and other parts used at elevated temperatures,long term usage below 900°C,short term usage temperature can reach 1080°C.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Substantial Temp Nickel Centered & Tremendous Alloys – Mechanical Homes Inconel Round Bar, Plate Sheet Offer – Inconel is designed of Mostly Nickel and a number of other aspects. The origin coming from Supernovas. Inconel is a Tremendous Alloy and Michlin Metals sells Inconel Round Bar, Hex Bar, Flat Bar, Plate, Sheet, Tube and Pipe.
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.1,Third Industrial District XiTou Village SongGang Town Bao’An District ShenZhen City GuangDong Province China