YG10C
YG10C Material grades and equivalents
|
Trademark |
UNS |
ISO |
AISI/ASTM |
|
YG10C |
|
|
|
Chemical composition(mass fraction)(%)
|
Alloy |
WC |
TiC |
TaC (NbC) |
Co |
Other |
|
YG10C |
90 |
- |
- |
10 |
Physical properties &minimum mechanical properties
|
Density/ g/cm |
Min Hardness/HRA |
Tensile strength/MPa |
Impact toughness j/cm |
Min Bending strength/ N/cm2 |
|
|
14.3-14.6 |
86 |
2300
|
- |
|
YG10C Characteristic as below:
It is a coarse grain tungsten carbide alloy with a slightly higher strength than YG15, and the wear resistance is better than that of YG15.
.YG10C Processing conditions and application:
A bit used for the percussion of a rotary drill and a drill for a rock drill; also used for a stamping die under general impact load.