Cemented carbide YG8C /ISO G15

\
Loading...

Short Introduction:

YG8C is a coarse grain tungsten carbide alloy, and its performance and wear resistance are similar to that of  YG11C. For percussive rotary drill bit. Cutting the teeth of a coal carrying machine with hard rock, an oil well drill, a hard stone processing tool, and a steel bar and steel tube stretching die for large compression rate.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    YG8C Material grades and equivalents: ISO G15

     Chemical composition(mass fraction)(%)                                                 

    Alloy

    WC

    TiC

    TaC  (NbC)

    Co

    Other

    YG8C

    92

    -

    -

    8

    -

     Physical properties &minimum mechanical properties

    Density/ g/cm

    Min Hardness/HRA

    Tensile strength/MPa

    Impact toughness j/cm

    Min Bending strength/ N/cm2

     
     
    14.5-14.9 88 1750

    3

    -  

    YG8C Characteristic as below:

    It is a coarse grain tungsten carbide alloy, and its performance and wear resistance are similar to that of YG11C.

    YG8C Processing conditions and application:

    For percussive rotary drill bit. Cutting the teeth of a coal carrying machine with hard rock, an oil well drill, a hard stone processing tool, and a steel bar and steel tube stretching die for large compression rate.

     

    Regular shape for all kinds of alloys

    Form

    Specification

    Supply Form

    Others

    Sheet

    Thickness:0.40-4.75mm,General Width:1000、1219、1500mm

    Whole Coil or piece of it

    Cold Annealed,Surface 2B、2E

    Plate

    Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled)

    Whole Coil or piece of it

    Single hot rolling,Solid solution annealed state,Surface 1D

    Belt

    Thickness:0.10-3.0mm,Width:50-500mm

    Whole Coil or Specified size

    Cold Annealed,Surface 2B、2E

    Bar & Rod

    Rolled barΦ5-45mm,Length≤1500mm

    Polished Bar(circle、Square)

    Solution annealing,descaling

    Forged barΦ26-245mm,Length≤4000mm

    Weld tube

    Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm

    Base on your requirement

    Seamless Tube

    Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm

    Base on your requirement

    Wire

    Outer diameterΦ0.1-13mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Forged piece

    discs,rings,squares,blocks,slabs

    Base on your requirement

    Steel, Alloy

    Flangs

    All kinds of Flangs

    Base on your requirement

    Steel, Alloy

    Welding Material

    Coil wire Φ0.025mm-1.6mm

    Base on your requirement

    Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.

    Straight WireΦ1.6mm-4.0mm

    Welding rodΦ1.2mm-4.0mm

    Tube

    Elbow, three links, four links, different diameter size

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Explosive bonded laminate

    Raw Sheet Thickness≥2mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy


  • Previous:
  • Next:

  • Write your message here and send it to us

    RELATED PRODUCTS

    WhatsApp Online Chat !