Cemented carbide YT15 /ISO P10

\
Loading...

Short Introduction:

YT15 compared with YT14, its wear resistance is improved, but its impact resistance is poor.It is suitable for continuous cutting of coarse steel, semi fine car and fine car during continuous cutting, for example, small section precision car for intermittent cutting, semi finish milling and finishing milling of continuous surface, rough expansion and fine enlargement of hole. Fine and semi fine milling for continuous cutting of carbon steel and alloy steel in continuous cutting, fine and coarse expansion of holes.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    YT15  Material grades and equivalents:ISO P10

    Chemical composition(mass fraction)(%)

    Alloy

    WC

    TiC

    TaC  (NbC)

    Co

    Other

    YT15

    79

    15

    -

    6

    -

    Physical properties &minimum mechanical properties

    Density/ g/cm

    Min Hardness/HRA

    Tensile strength/MPa

    Impact toughness j/cm

    Min Bending strength/ N/cm2

    11.0-12.7

    91

    1150

    -

    1150

    YT15 Characteristic as below:

    Compared with YT14, its wear resistance is improved, but its impact resistance is poor.

    YT15 Processing conditions and application:

    It is suitable for continuous cutting of coarse steel, semi fine car and fine car during continuous cutting, for example, small section precision car for intermittent cutting, semi finish milling and finishing milling of continuous surface, rough expansion and fine enlargement of hole. Fine and semi fine milling for continuous cutting of carbon steel and alloy steel in continuous cutting, fine and coarse expansion of holes.

     

    Regular shape for all kinds of alloys

    Form

    Specification

    Supply Form

    Others

    Sheet

    Thickness:0.40-4.75mm,General Width:1000、1219、1500mm

    Whole Coil or piece of it

    Cold Annealed,Surface 2B、2E

    Plate

    Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled)

    Whole Coil or piece of it

    Single hot rolling,Solid solution annealed state,Surface 1D

    Belt

    Thickness:0.10-3.0mm,Width:50-500mm

    Whole Coil or Specified size

    Cold Annealed,Surface 2B、2E

    Bar & Rod

    Rolled barΦ5-45mm,Length≤1500mm

    Polished Bar(circle、Square)

    Solution annealing,descaling

    Forged barΦ26-245mm,Length≤4000mm

    Weld tube

    Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm

    Base on your requirement

    Seamless Tube

    Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm

    Base on your requirement

    Wire

    Outer diameterΦ0.1-13mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Forged piece

    discs,rings,squares,blocks,slabs

    Base on your requirement

    Steel, Alloy

    Flangs

    All kinds of Flangs

    Base on your requirement

    Steel, Alloy

    Welding Material

    Coil wire Φ0.025mm-1.6mm

    Base on your requirement

    Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.

    Straight WireΦ1.6mm-4.0mm

    Welding rodΦ1.2mm-4.0mm

    Tube

    Elbow, three links, four links, different diameter size

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Explosive bonded laminate

    Raw Sheet Thickness≥2mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy


  • Previous:
  • Next:

  • Write your message here and send it to us