Cemented carbide YW2/ ISO M20

\

Short Introduction:

YW2 is the wear resistance of steel products is higher than that of class YG alloys. When processed iron and non-ferrous metals and alloys, the impact toughness is poor, and the effect is not better than that of class YG alloy.It is suitable for finishing and semi finishing of special refractory steel, such as heat-resistant steel, high manganese steel, stainless steel and high alloy steel. The processing of ordinary steel and cast iron. Used for rough machining of heat resistant steel, high manganese steel and high alloy steel and other hard steel processing and semi finishing machining.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    YW2  Material grades and equivalents:ISO M20

    Chemical composition(mass fraction)(%)

    Alloy

    WC

    TiC

    TaC  (NbC)

    Co

    Other

    YW2

    82-83

    6

    3~4

    8

    Physical properties &minimum mechanical properties

    Density/ g/cm

    Min Hardness/HRA

    Tensile strength/MPa

    Impact toughness j/cm

    Min Bending strength/ N/cm2

    12.4-13.5

    90.5

    1350

    -

    1350

    YW2 Characteristic as below:

    The wear resistance of steel products is higher than that of class YG alloys. When processed iron and non-ferrous metals and alloys, the impact toughness is poor, and the effect is not better than that of class YG alloy.

    YW2 Processing conditions and application:

    It is suitable for finishing and semi finishing of special refractory steel, such as heat-resistant steel, high manganese steel, stainless steel and high alloy steel. The processing of ordinary steel and cast iron. Used for rough machining of heat resistant steel, high manganese steel and high alloy steel and other hard steel processing and semi finishing machining.

    Regular shape for all kinds of alloys

    Form

    Specification

    Supply Form

    Others

    Sheet

    Thickness:0.40-4.75mm,General Width:1000、1219、1500mm

    Whole Coil or piece of it

    Cold Annealed,Surface 2B、2E

    Plate

    Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled)

    Whole Coil or piece of it

    Single hot rolling,Solid solution annealed state,Surface 1D

    Belt

    Thickness:0.10-3.0mm,Width:50-500mm

    Whole Coil or Specified size

    Cold Annealed,Surface 2B、2E

    Bar & Rod

    Rolled barΦ5-45mm,Length≤1500mm

    Polished Bar(circle、Square)

    Solution annealing,descaling

    Forged barΦ26-245mm,Length≤4000mm

    Weld tube

    Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm

    Base on your requirement

    Seamless Tube

    Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm

    Base on your requirement

    Wire

    Outer diameterΦ0.1-13mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Forged piece

    discs,rings,squares,blocks,slabs

    Base on your requirement

    Steel, Alloy

    Flangs

    All kinds of Flangs

    Base on your requirement

    Steel, Alloy

    Welding Material

    Coil wire Φ0.025mm-1.6mm

    Base on your requirement

    Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.

    Straight WireΦ1.6mm-4.0mm

    Welding rodΦ1.2mm-4.0mm

    Tube

    Elbow, three links, four links, different diameter size

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Explosive bonded laminate

    Raw Sheet Thickness≥2mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy


  • Previous:
  • Next:

  • Write your message here and send it to us