6J22 precision alloy

\

Short Introduction:

6J22 precision alloy is nickel, chromium, aluminum, iron as the main ingredient. The resistivity is about three times higher than that of manganese and copper, and has a lower temperature coefficient of resistance and low copper thermoelectric power, with good resistance to long-term stability and oxidation resistance, the use of a wide temperature range.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    Short Introduction:

    6J22 precision alloy is nickel, chromium, aluminum, iron as the main ingredient. The resistivity is about three times higher than that of manganese and copper, and has a lower temperature coefficient of resistance and low copper thermoelectric power, with good resistance to long-term stability and oxidation resistance, the use of a wide temperature range.

    6J22 Material grades and equivalents

    KAMA 6J22/ 2.4872/ NiCr20AISi

     

    6J22 chemical ingredients:

    Alloy

    %

    Cr

    P

    S

    Ni

    Al

    C

    Mn

    Si

    Fe

    6J22

    Min

    19

    Rest

    2.7

    0.5

    2.0

    Max

    21.5

    0.010

    0.010

    3.2

    0.04

    1.5

    0.2

    3.0

     

    6J22 Precision Alloy Applications Applications:

    Applicable to the production of various measuring instruments, precision instruments in the resistance components.

    Suitable for the production of precision micro-resistance components and strain gauges.

    Metal materials to find the problem Shenzhen Hua Ni special alloy. Nickel nickel concentrate on solving the user products in high temperature, high corrosion, high creep, high strength, high hardness, high wear resistance and high temperature corrosion-resistant capillary and other complex environment conditions Metallic material problems.

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy