Iron alloy Stainless Steel Nitronic 50

\

Short Introduction:

HY Nitronic 50/S20910/XM-19/ Fxm-19/Nitronic50 Stainless Steel provides a combination of corrosion resistance and strength not found in any other commercial material.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY Nitronic 50  Material grades and equivalents

    UNS

    AISI/ASTM

    ID

    Trademark

    S20910

    XM-19

    Fxm-19

    Nitronic50

     HY Nitronic 50 Chemical composition:

    Alloy

    %

    Ni

    Cr

    Fe

    C

    Mn

    Si

    N

    Mo

    Nb

    V

    P

    S

    HY Nitronic 50

    Min.

    11.5

    20.5

    52

    4

    0.2

    1.5

    0.1

    0.1

    Max.

    13.5

    23.5

    62

    0.06

    6

    1

    0.4

    3

    0.3

    0.3

    0.04

    0.03

     HY Nitronic 50 Physical properties

    Density

    7.8g/cm3

    Melting point

    1415-1450 °C

     HY Nitronic 50 Alloy mi nimum mechanical properties in the room temperature

    Alloy status

    Tensile strength

    Rm N/mm²

    Yield strength

    RP0.2 N/mm²

    Elongation

    A5 %

    Brinell hardness

    HB

    Solution treatment

    690

    380

    35

    ≤241

     HY Nitronic 50 Characteristic:

    HY Nitronic 50 Stainless Steel provides a combination of corrosion resistance and strength not found in any other commercial material. This austenitic stainless steel has corrosion resistance greater than that provided by types 316, 316L, 317, 317L plus approximately twice the yield strength at room temperature. In addition, HY Nitronic 50 has very good mechanical properties at both elevated and sub-zero temperatures unlike many austenitic stainless steel grades.

    HY Nitronic 50 does not become magnetic in cryogenic situations.

    High Strength (HS) Nitronic 50 has a yield strength about three times that of 316 Stainless Steel.

    HY Nitronic 50 Application field:

    Used in petroleum, petrochemical, manure, chemical, nuclear fuel recycle, paper making, textile and food processing industries parts of furnace, combustion chamber, gas turbine and heat-treating facility connecting piece

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy



  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !