Cemented carbide YG15/ ISOK40、G30

\

Short Introduction:

YG15 ,the wear resistance is lower than that of the above alloy.It is suitable for the drawing of steel bars and steel tubes under high compression, and the forging, punching and stamping tools working under large stress. Drills for impact rotary drilling machines; steel bars, drawing dies and stamping tools for qmq pipes.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    YG15  Material grades and equivalents

    Trademark

    UNS

    ISO

    AISI/ASTM

    YG15

    K40/G30

    Chemical composition(mass fraction)(%)

    Alloy

    WC

    TiC

    TaC  (NbC)

    Co

    Other

    YG15

    85

    -

    15

    Physical properties &minimum mechanical properties

    Density/ g/cm

    Min Hardness/HRA

    Tensile strength/MPa

    Impact toughness j/cm

    Min Bending strength/ N/cm2

    13.9-14.2

    87

    2100

    4-

    YG15 Characteristic as below:

    The wear resistance is lower than that of the above alloy.

    YG15 Processing conditions and application:

    It is suitable for the drawing of steel bars and steel tubes under high compression, and the forging, punching and stamping tools working under large stress. Drills for impact rotary drilling machines; steel bars, drawing dies and stamping tools for qmq pipes.