Cemented carbide YG3

\

Short Introduction:

YG3 is a kind of alloy with the highest wear resistance in tungsten cobalt alloy, but its impact toughness is poor. For cast iron, non-ferrous metal and alloy precision boring and fine car, also used for finishing of hardened steel and tungsten steel, and wire drawing die.It is suitable for high speed finishing of small cutting section of cast iron, nonferrous metal and alloy hardened steel alloy steel.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    YG3  Material grades and equivalents

    Chemical composition(mass fraction)(%)

    Alloy

    WC

    TiC

    TaC  (NbC)

    Co

    Other

    YG3

    97

    -

    -

    3

    -

    Physical properties &minimum mechanical properties

    Density/ g/cm

    Min Hardness/HRA

    Tensile strength/MPa

    Impact toughness j/cm

    Min Bending strength/ N/cm2

    15.0-15.3

    91

    1200

    -

    -

    YG3 Characteristic as below:

    A kind of alloy with the highest wear resistance in tungsten cobalt alloy, but its impact toughness is poor. For cast iron, non-ferrous metal and alloy precision boring and fine car, also used for finishing of hardened steel and tungsten steel, and wire drawing die.

    YG3 Processing conditions and application:

     It is suitable for high speed finishing of small cutting section of cast iron, nonferrous metal and alloy hardened steel alloy steel.

    Regular shape for all kinds of alloys

    Form

    Specification

    Supply Form

    Others

    Sheet

    Thickness:0.40-4.75mm,General Width:1000、1219、1500mm

    Whole Coil or piece of it

    Cold Annealed,Surface 2B、2E

    Plate

    Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled)

    Whole Coil or piece of it

    Single hot rolling,Solid solution annealed state,Surface 1D

    Belt

    Thickness:0.10-3.0mm,Width:50-500mm

    Whole Coil or Specified size

    Cold Annealed,Surface 2B、2E

    Bar & Rod

    Rolled barΦ5-45mm,Length≤1500mm

    Polished Bar(circle、Square)

    Solution annealing,descaling

    Forged barΦ26-245mm,Length≤4000mm

    Weld tube

    Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm

    Base on your requirement

    Seamless Tube

    Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm

    Base on your requirement

    Wire

    Outer diameterΦ0.1-13mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Forged piece

    discs,rings,squares,blocks,slabs

    Base on your requirement

    Steel, Alloy

    Flangs

    All kinds of Flangs

    Base on your requirement

    Steel, Alloy

    Welding Material

    Coil wire Φ0.025mm-1.6mm

    Base on your requirement

    Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.

    Straight WireΦ1.6mm-4.0mm

    Welding rodΦ1.2mm-4.0mm

    Tube

    Elbow, three links, four links, different diameter size

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Explosive bonded laminate

    Raw Sheet Thickness≥2mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy


  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !